| Category: | PP Homopolymer , Polypropylene Homopolymer |
| Manufacturer: | SIBUR, LLC |
| Trademark: | TOLEN |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | YZVvDb_TOLEN-H080-GP.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| PP H080 GP is a polypropylene homopolymer with standard molecular mass distribution. The product features fluidity above average, an optimal stabilization package and balanced physical and mechanical properties. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 8.0 | g/10 min | Internal Method |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress 1(Yield) | 30.0 | MPa | Internal Method |
| Tensile Strain 2(Yield) | 10 | % | Internal Method |
| Flexural Modulus 3 | 1400 | MPa | Internal Method |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength (23°C) | 2.0 | kJ/m² | Internal Method |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (0.45 MPa, Unannealed) | 80.0 | °C | Internal Method |
| Vicat Softening Temperature | 155 | °C | Internal Method 4 |
| Note Message | |
|---|---|
| 1 . | 50 mm/min |
| 2 . | 50 mm/min |
| 3 . | 5.0 mm/min |
| 4 . | A (10N) |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| 3M™ Dyneon™ PTFE TF 2025Z | 3M Advanced Materials Division | PTFE | 3M™ Dyneon™ PTFE |
| ADEKA Y65-55 | Adeka Corporation | PUR-Ester | ADEKA |
| Kumho PS HI 425E | Korea Kumho Petrochemical Co., Ltd. | PS (HIPS) | Kumho PS |
| ISPLEN® PB 171 H1M | REPSOL | PP Impact Copolymer | ISPLEN® |
| Jampilen EP200M | Jam Polypropylene Company | PP Copolymer | Jampilen |