| Category: | SMA , Styrene Maleic Anhydride |
| Manufacturer: | Polyscope Polymers BV |
| Trademark: | XIRAN® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | Y4sXac_XIRAN-SZ15170.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
XIRAN® SZ15170 is an amorphous thermoplastic random SMA (styrene maleic anhydride) copolymer. XIRAN® SZ15170 is typically added to other engineering plastics to increase:
Application areas XIRAN® SZ15170 is specifically designed to be used in film extrusion applications or in combination with an impact modifier like ABS or HIPS as an extrusion or injection molding grade. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.12 | g/cm³ | ISO 1183 |
| Apparent Density | 0.60 | g/cm³ | Internal method |
| Maleic Anhydride Content | 15 | % | Internal method |
| Molecular Weight | 170000 | g/mol | Internal method |
| Moisture Content | ppm | ISO 760 |
| Additional Information | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Pellet Size | 4.00 | mm | |
| Polydispersity - (Mw/Mn) | 2.50 | ISO 13885-1 | |
| Volatiles | ppm | GC |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Glass Transition Temperature | 130 | °C | ISO 3146 |
| Vicat Softening Temperature | 125 | °C | ISO 306 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 80.0 - 90.0 | °C | |
| Drying Time | 2.0 - 3.0 | hr | |
| Rear Temperature | 210 - 240 | °C | |
| Middle Temperature | 210 - 240 | °C | |
| Front Temperature | 210 - 240 | °C | |
| Processing (Melt) Temp | < 280 | °C |
| Injection instructions |
|---|
| Optimum processing temperature: 220-260°C |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 80.0 - 90.0 | °C | |
| Drying Time | 2.0 - 3.0 | hr | |
| Cylinder Zone 1 Temp. | 210 - 240 | °C | |
| Cylinder Zone 2 Temp. | 210 - 240 | °C | |
| Cylinder Zone 3 Temp. | 210 - 240 | °C | |
| Cylinder Zone 4 Temp. | 210 - 240 | °C | |
| Cylinder Zone 5 Temp. | 210 - 240 | °C |
| Extrusion instructions |
|---|
| Optimum processing temperature: 220-260°CMaximum processing temperature: 280°C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 700 | RTP Company | HDPE | RTP |
| Radilon® AGV 15 Natural | Radici Plastics | Nylon 66 | Radilon® |
| Keliren® CPE402 | Hangzhou Keli Chemical Co., Ltd. | CPE | Keliren® |
| LOXIM 841 02T HB | LOXIM Industries Private Limited | PP Copolymer | LOXIM |
| Edgetek™ AS-20GF/000 BLACK | PolyOne Corporation | ABS | Edgetek™ |