| Category: | PP Copolymer , Polypropylene Copolymer |
| Manufacturer: | MBA Polymers |
| Trademark: | MBA PP |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | Y3GdcL_MBA-PP-2117.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| A post-consumer recycled polypropylene copolymer for general use. Available in standard black (reference 90/04). |
| General Information | |
|---|---|
| Recycled Content |
|
| Features |
|
| Uses |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.940 | g/cm³ | Internal Method |
| Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 7.5 | g/10 min | ISO 1133 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Yield, 23°C) | 21.0 | MPa | ISO 527-2/50 |
| Flexural Modulus (23°C) | 870 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength (23°C) | 6.0 | kJ/m² | ISO 180/1A |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 80.0 | °C | |
| Drying Time | 1.0 to 2.0 | hr | |
| Suggested Max Moisture | 0.050 to 0.10 | % | |
| Processing (Melt) Temp | 190 to 220 | °C | |
| Mold Temperature | 30.0 to 60.0 | °C |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 80.0 | °C | |
| Drying Time | 1.0 to 2.0 | hr | |
| Suggested Max Moisture | 0.050 to 0.10 | % | |
| Melt Temperature | 180 to 210 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| TAROMID B 280 G4 | Taro Plast S.p.A. | Nylon 6 | TAROMID B |
| VESTAMID® L LX9012 | Evonik Industries AG | Nylon 12 | VESTAMID® L |
| Witcobond® W-244 | Chemtura | PUR-Ester | Witcobond® |
| ExxonMobil™ PP7075L1 | ExxonMobil Chemical | PP Impact Copolymer | ExxonMobil™ |
| Lifoflex® UV 90 GA 1090 | ELASTO | SEBS | Lifoflex® |