| Category: | Nylon 66 , Polyamide 66 |
| Manufacturer: | Teknor Apex Company (Chem Polymer) |
| Trademark: | Chemlon® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | XavR8m_Chemlon-130-M.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Chemlon® 130 M is a Polyamide 66 (Nylon 66) material filled with 30% mineral. It is available in Asia Pacific, Europe, or North America for injection molding. Primary attribute of Chemlon® 130 M: Warp Resistant. |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Features |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.40 | g/cm³ | ASTM D792 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength (23°C) | 96.5 | MPa | ASTM D638 |
| Tensile Elongation (Break, 23°C) | 2.0 | % | ASTM D638 |
| Flexural Modulus (23°C) | 4140 | MPa | ASTM D790 |
| Flexural Strength (23°C) | 124 | MPa | ASTM D790 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact (23°C) | 48 | J/m | ASTM D256 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Deflection Temperature Under Load (1.8 MPa, Unannealed) | 199 | °C | ASTM D648 |
| Melting Temperature | 254 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 1300 C GB 40 | RTP Company | PPS | RTP |
| Yuyao PPO GFN2-501 | Yuyao Tenglong Plastics Co., Ltd. | PPE+PS | Yuyao PPO |
| EPO-TEK® H31LV | Epoxy Technology Inc. | Epoxy | EPO-TEK® |
| ICORENE® 4140 | ICO Polymers SA, A Division of A. Schulman | PE Copolymer | ICORENE® |
| Deprene 203-50 | Shanghai Lin Gen Rubber Materials Co., Ltd. | PP+EPDM | Deprene |