Category: | Nylon 66 , Polyamide 66 |
Manufacturer: | Solvay Engineering Plastics |
Trademark: | TECHNYL® A |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | Xa5bsO_TECHNYL-A-30H1-V25-NATURAL.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Flame-retardant polyamide 66, 25% glass-fibre reinforced, heat stabilized for injection moulding. |
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Uses |
|
Appearance |
|
Processing Method |
|
Part Marking Code (ISO 11469) |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.54 | -- | g/cm³ | ISO 1183/A |
Water Absorption (23°C, 24 hr) | 0.0 | -- | % | ISO 62 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus | 8800 | 7000 | MPa | ISO 527-2/1A |
Tensile Stress (Break) | 95.0 | 78.0 | MPa | ISO 527-2/1A |
Tensile Strain (Break) | 2.5 | 3.0 | % | ISO 527-2/1A |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength | 9.0 | 10 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength | 45 | 47 | kJ/m² | ISO 179/1eU |
Notched Izod Impact Strength | 9.8 | 11 | kJ/m² | ISO 180/1A |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 220 | -- | °C | ISO 75-2/Af |
Melting Temperature | 263 | -- | °C | ISO 11357-3 |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Comparative Tracking Index (Solution A) | 500 | 600 | V | IEC 60112 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Flame Rating | UL 94 | |||
0.800 mm | V-0 | -- | ||
1.60 mm | V-0 | -- | ||
3.20 mm | V-0 | -- | ||
Glow Wire Flammability Index | IEC 60695-2-12 | |||
0.800 mm | 960 | -- | °C | |
1.60 mm | 960 | -- | °C | |
Glow Wire Ignition Temperature | IEC 60695-2-13 | |||
0.800 mm | 775 | -- | °C | |
1.60 mm | 775 | -- | °C |
Injection | Dry | Unit | |
---|---|---|---|
Drying Temperature | 80.0 | °C | |
Suggested Max Moisture | 0.20 | % | |
Rear Temperature | 275 to 280 | °C | |
Middle Temperature | 280 to 285 | °C | |
Front Temperature | 285 to 290 | °C | |
Mold Temperature | 60.0 to 90.0 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
SABIC® PP PHC26 | Saudi Basic Industries Corporation (SABIC) | PP Impact Copolymer | SABIC® PP |
SOLARENE DM100 | Dongbu Hannong Chemical | PS (GPPS) | SOLARENE |
Skyrol® SL70 | SKC Inc. | PET | Skyrol® |
NITRIFLEX NP-6021 | NITRIFLEX | NBR | NITRIFLEX |
Latan 13 K/30 | LATI S.p.A. | Acetal (POM) Copolymer | Latan |