FX-8071 is a flexible polyurethane formulated for room temperature hand-batch systems. Excellent physical properties can be obtained without the utilization of mercury, MOCA, or TDI. FX-8071 meets the criteria to pass UL 94VO. |
General Information | |
---|---|
Features |
|
Appearance |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | |||
Hardener | 1.22 | g/cm³ | |
Cured | 1.30 | g/cm³ | |
Base Resin | 1.30 | g/cm³ | |
Molding Shrinkage - Flow | 0.10 to 0.50 | % | ASTM D2566 |
Thermoset | Nominal Value | Unit | Test Method |
---|---|---|---|
Thermoset Components | |||
Hardener | Mix Ratio by Volume: 100 Mix Ratio by Weight: 100 | ||
Resin | Mix Ratio by Weight: 39 Mix Ratio by Volume: 37 | ||
Demold Time | 120 to 240 | min |
Uncured Properties | Nominal Value | Unit | Test Method |
---|---|---|---|
Viscosity | |||
25°C 1 | 0.32 | Pa·s | |
25°C 2 | 1.9 | Pa·s | |
25°C 3 | 1.9 | Pa·s | |
Curing Time (25°C) | 1.7E+2 | hr | |
Gel Time | 10 to 15 | min |
Cured Properties | Nominal Value | Unit | Test Method |
---|---|---|---|
Shore Hardness (Shore A) | 65 to 75 | ASTM D2240 | |
Tensile Strength | 4.14 | MPa | ASTM D638 |
Tensile Elongation at Break | 150 | % | ASTM D638 |
Tear Strength | 15.1 | kN/m | ASTM D624 |
Note Message | |
---|---|
1 . | Resin |
2 . | Mixed |
3 . | Hardener |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Thermx® LED 0201S | Celanese Corporation | PCT | Thermx® |
Torelina® A503-F1 | Toray Resin Company | PPS | Torelina® |
Dyflor EE | Evonik Industries AG | PVDF | Dyflor |
Lupoy® SC1004L | LG Chem Ltd. | PC | Lupoy® |
Nylux 66-NAT | KMI Group, Inc. | Nylon 66 | Nylux |