| Category: | TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester) |
| Manufacturer: | Lubrizol Advanced Materials, Inc. |
| Trademark: | Estane® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | XHSo3b_Estane-ETE-60DS3-TPU.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Type: Estane® ETE 60DS3 is a 60D aromatic Polyester-Based Thermoplastic Polyurethane (TPU). Features: Hard TPU with wide extrusion processing window and melt stability, high transparency Uses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket; Injection molding: Various |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| RoHS Compliance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.23 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore D, 5 sec) | 57 - 63 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Taber Abrasion Resistance (1000 Cycles, 1000 g, H-18 Wheel) | 62.0 | mg | ASTM D3389 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ASTM D412 | ||
| 100% strain, 0.762mm | 23.0 | MPa | ASTM D412 |
| 300% strain, 0.762mm | 49.0 | MPa | ASTM D412 |
| Tensile Strength (Break, 0.762 mm) | 49.0 | MPa | ASTM D412 |
| Tensile Elongation (Break, 0.762 mm) | 300 | % | ASTM D412 |
| Tear Strength | |||
| 0.762 mm 1 | 175 | kN/m | ASTM D624 |
| Cracking | 35 | kN/m | ASTM D470 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Glass Transition Temperature | -18.0 | °C | DSC |
| Melting Temperature | 172 | °C | DSC |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 104 | °C | |
| Drying Time | 2.0 - 4.0 | hr | |
| Suggested Max Moisture | 0.020 | % | |
| Cylinder Zone 1 Temp. | 199 | °C | |
| Cylinder Zone 2 Temp. | 204 | °C | |
| Cylinder Zone 3 Temp. | 204 | °C | |
| Cylinder Zone 4 Temp. | 210 | °C | |
| Adapter Temperature | 213 | °C | |
| Melt Temperature | 204 | °C | |
| Die Temperature | 210 | °C |
| Extrusion instructions |
|---|
| Dew Point: -40°CScreen Pack Recommendation: 20/40/80/20 |
| Note Message | |
|---|---|
| 1 . | C mould |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| SLOVALEN® PH 32 T 20 | Plastcom | PP, Unspecified | SLOVALEN® |
| Bergamid™ A700 G25 H (f1) | PolyOne Corporation | Nylon 66 | Bergamid™ |
| Borcoat™ MA115E | Borealis AG | PP, Unspecified | Borcoat™ |
| INEOS LLDPE LL6910KJ | INEOS Olefins & Polymers Europe | LLDPE | INEOS LLDPE |
| Formolene® 3310Z | Formosa Plastics Corporation, U.S.A. | PP Random Copolymer | Formolene® |