Category: | PUR-Ether/TDI , Polyurethane (Polyether, TDI) |
Manufacturer: | Anderson Development Company |
Trademark: | Andur |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | X766Tb_Andur-6500-AP-Curene-280.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
All properties based on Andur® 6500-5AP cured with Curene® 280 |
General Information | |
---|---|
Forms |
|
Processing Method |
|
Hardness | Nominal Value | Test Method | |
---|---|---|---|
Durometer Hardness (Shore A) | 92 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | 23.6 | MPa | ASTM D638 |
Tensile Elongation (Break) | 270 | % | ASTM D638 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (100% Strain) | 9.10 | MPa | ASTM D412 |
Tear Strength | |||
-- 1 | 64.8 | kN/m | ASTM D624 |
Cracking | 21 | kN/m | ASTM D470 |
Compression Set | 31 | % | ASTM D395 |
Thermoset | Nominal Value | Unit | |
---|---|---|---|
Pot Life | 4.0 | min | |
Post Cure Time (23°C) | 72 | hr |
Additional Information |
---|
Prepolymer NCO%: 7.6-8.2Grams Curene® 280 per 100 grams prepolymer: 49.4Rebound, %: 35Stoichiometry: 0.95Prepolymer Temperature, °F: 190-210Curene® 280 Temperature, °F: 158Post Cure Time, 212°F, hours: 16 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Mold Temperature | 107 | °C |
Note Message | |
---|---|
1 . | C mould |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 207 MS HS | RTP Company | Nylon 66 | RTP |
Reny® 1071 | Mitsubishi Engineering-Plastics Corp | PARA | Reny® |
Axplas® MEP52 7081 | Axion Polymers | TP, Unspecified | Axplas® |
ALTECH® PA66 ECO 1000/506 | ALBIS PLASTIC GmbH | Nylon 66 | ALTECH® PA66 |
TechnoMid PA6 S GF 15 | TechnoCompound GmbH | Nylon 6 | TechnoMid |