Category: | TPV , Thermoplastic Vulcanizate |
Manufacturer: | Taro Plast S.p.A. |
Trademark: | TAROPRENE® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | X6nmnh_TAROPRENE-1-A75-M1N.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Thermoplastic Elastomer Vulcanized. This TPE-V compound combines the typical performance of a vulcanized elastomer with the easy processing of a thermoplastic compound. Taroprene is totally recyclable and it can be produced in standard grades and in tailor-made grades. Available in natural, black and colored grade. |
General Information | |
---|---|
Features |
|
Appearance |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.960 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (190°C/5.0 kg) | 3.0 | g/10 min | ISO 1133 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Shore Hardness (Shore A, 3 sec) | 75 | ISO 868 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress 1 | ASTM D412 | ||
100% Strain | 3.20 | MPa | |
300% Strain | 5.30 | MPa | |
Tensile Strength 2(Break) | 7.40 | MPa | ASTM D412 |
Tensile Elongation 3(Break) | 500 | % | ASTM D412 |
Tear Strength | 28.0 | kN/m | ASTM D624 |
Compression Set | ASTM D395B | ||
70°C, 22 hr | 37 | % | |
100°C, 22 hr | 42 | % |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 80.0 | °C | |
Drying Time | 2.0 | hr | |
Processing (Melt) Temp | 170 to 230 | °C |
Note Message | |
---|---|
1 . | Die C |
2 . | Die C |
3 . | Die C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 2100 GB 20 | RTP Company | PEI | RTP |
SILPURAN® 8060/50 | Wacker Chemie AG | Silicone | SILPURAN® |
Huafon JF-P-9186 / JF-I-9422 | Huafon Group Co., Ltd. | PUR-Ester | Huafon |
Petrothene® GA503028 | LyondellBasell Industries | LLDPE | Petrothene® |
PLUSTEK PB306G6 | Polyram Ram-On Industries | Nylon 6 | PLUSTEK |