| Category: | Nylon 11 , Polyamide 11 |
| Manufacturer: | Arkema |
| Trademark: | Rilsan® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | Wq6dPn_Rilsan-BESHV.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Rilsan® BESHV is a Polyamide 11 (Nylon 11) product. It can be processed by extrusion, film extrusion, injection molding, or profile extrusion and is available in Africa & Middle East, Asia Pacific, Europe, Latin America, or North America. Characteristics include:
|
| General Information | |
|---|---|
| Additive |
|
| Features |
|
| Forms |
|
| Processing Method |
|
| Multi-Point Data |
|
| Physical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Density | 1030 | 1030 | kg/m³ | ISO 1183 1 |
| Melt volume-flow rate (235°C/10.0 kg) | 1.00 | -- | cm³/10min | ISO 1133 2 |
| Water Absorption (Saturation) | 1.9 | -- | % | ISO 62 3 |
| Mechanical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Tensile modulus | 1360 | 1200 | MPa | ISO 527-2 4 |
| Tensile Stress (Yield) | 40.0 | 37.0 | MPa | ISO 527-2 5 |
| Tensile Strain (Yield) | 5.0 | 22 | % | ISO 527-2 6 |
| Nominal strain at break | > 50 | > 50 | % | ISO 527-2 7 |
| Impact | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Charpy notched impact strength | ISO 179/1eA 8 | |||
| -30°C | 11.0 | 15.0 | kJ/m² | |
| 23°C | -- | 32.0 | kJ/m² | |
| Charpy impact strength | ISO 179/1eU 9 | |||
| -30°C | No Break | No Break | ||
| 23°C | No Break | No Break | ||
| Puncture energy (-30°C) | -- | 75.0 | J | ISO 6603-2 10 |
| Puncture - maximum force (-30°C) | -- | 6800 | N | ISO 6603-2 11 |
| Thermal | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Deflection Temperature Under Load | ISO 75-2 12 | |||
| 0.45 MPa | 145 | -- | °C | |
| 1.8 MPa | 50.0 | -- | °C | |
| Vicat Softening Temperature (50°C/h, B (50N)) | 160 | -- | °C | ISO 306 13 |
| Melting Temperature 14 | 189 | -- | °C | ISO 11357-3 15 |
| CLTE - Flow | 8.5E-5 | -- | cm/cm/°C | ISO 11359-2 16 |
| Electrical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Surface resistivity | -- | 1.0E+14 | ohms | IEC 60093 17 |
| Volume resistivity | -- | 1.0E+12 | ohms·m | IEC 60093 18 |
| Electric strength | -- | 30 | kV/mm | IEC 60243-1 19 |
| Flammability | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Burning Behav. at 1.6mm nom. thickn. (1.60 mm) | V-2 | -- | ISO 1210 20 | |
| Burning Behav. at thickness h (3.20 mm) | V-2 | -- | ISO 1210 21 | |
| Oxygen index | 25 | -- | % | ISO 4589-2 22 |
| Note Message | |
|---|---|
| 1 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 2 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 3 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 4 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 5 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 6 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 7 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 8 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 9 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 10 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 11 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 12 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 13 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 14 . | 10 °C/min |
| 15 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 16 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 17 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 18 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 19 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 20 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 21 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 22 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| TAROLOX 10 K4 | Taro Plast S.p.A. | PBT | TAROLOX |
| Allen ABS 3800/LXS | SEKISUI Polymer Innovations, LLC | ABS | Allen ABS |
| Ferro PP MPP20FJ11NA | Ferro Corporation | PP Homopolymer | Ferro PP |
| LNP™ LUBRICOMP™ QL002 compound | SABIC Innovative Plastics | Nylon 610 | LNP™ LUBRICOMP™ |
| Sylvin 9940-75 NATURAL | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |