Wellamid® FRGF25-66 NBK3 is a Polyamide 66 (Nylon 66) material filled with 25% glass fiber. It is available in Asia Pacific, Europe, Latin America, or North America for injection molding. Important attributes of Wellamid® FRGF25-66 NBK3 are:
Typical application of Wellamid® FRGF25-66 NBK3: Automotive |
General Information | |
---|---|
Filler / Reinforcement |
|
Features |
|
Uses |
|
Appearance |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.48 | g/cm³ | ISO 1183 |
Molding Shrinkage | ISO 294-4 | ||
Across Flow : 23°C | 0.80 to 1.2 | % | |
Flow : 23°C | 0.30 to 0.70 | % |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (Yield, 23°C) | 115 | MPa | ISO 527-2 |
Tensile Strain (Yield, 23°C) | 3.0 | % | ISO 527-2 |
Flexural Modulus (23°C) | 7100 | MPa | ISO 178 |
Flexural Stress (23°C) | 165 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact Strength (23°C) | 6.0 | kJ/m² | ISO 180 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 240 | °C | ISO 75-2/A |
Melting Temperature | 260 | °C | ISO 3146 |
Flammability | Nominal Value | Test Method | |
---|---|---|---|
Flame Rating (0.800 mm) | V-0 | UL 94 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
megol® PUG 60 | API SpA | SEBS | megol® |
Novodur® H701 | Styrolution | ABS | Novodur® |
4LEX® 10F13301 | 4Plas | PC | 4LEX® |
Durethan® B 40 FA 000000 | LANXESS GmbH | Nylon 6 | Durethan® |
KOPA® KN3321G10V0L | Kolon Plastics, Inc. | Nylon 66 | KOPA® |