TECHNYL® A 218HP V30 BLACK 21N

Category: Nylon 66 , Polyamide 66
Manufacturer: Solvay Engineering Plastics
Trademark: TECHNYL®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: WgI4K7_TECHNYLA218HPV30BLACK21N.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
TECHNYL® A 218HP V30 Black 21N is a polyamide 6.6, reinforced with 30% of glass fiber, heat stabilized, for injection moulding. This grade is designed to offer a long term heat resistance and is suitable to work in environments characterized by a very high temperature. (200°C)
General Information
Filler / Reinforcement
  • Glass fiber reinforced material, 30% filler by weight
Additive
  • heat stabilizer
Features
  • Heat Stabilized - Inorganic
  • Good liquidity
Uses
  • Application in Automobile Field
Agency Ratings
  • EC 1907/2006 (REACH)
RoHS Compliance
  • RoHS compliance
Appearance
  • Black
Forms
  • Particle
Processing Method
  • Injection molding
Multi-Point Data
  • Isothermal Stress vs. Strain (ISO 11403-1)
Resin ID (ISO 1043)
  • PA66-GF30
PhysicalDryConditionedUnitTest Method
Density 1.35--g/cm³ISO 1183/A
MechanicalDryConditionedUnitTest Method
Tensile Modulus (23°C)100006600MPaISO 527-2/1A
Tensile Stress (Break, 23°C)170110MPaISO 527-2/1A
Tensile Strain (Break, 23°C)2.66.5%ISO 527-2
Flexural Modulus (23°C)90005900MPaISO 178
Flexural Stress (23°C)260180MPaISO 178
ImpactDryConditionedUnitTest Method
Charpy Notched Impact Strength (23°C)1418kJ/m²ISO 179/1eA
Charpy Unnotched Impact Strength (23°C)7877kJ/m²ISO 179/1eU
ThermalDryConditionedUnitTest Method
Heat Deflection Temperature
     0.45 MPa, not annealed 258--°CISO 75-2/Bf
     1.8 MPa, not annealed 245--°CISO 75-2/Af
Melting Temperature 262--°CISO 11357-3
InjectionDryUnit
Drying Temperature 80°C
Suggested Max Moisture 0.20%
Rear Temperature 270 - 280°C
Middle Temperature 275 - 285°C
Front Temperature 280 - 290°C
Mold Temperature 70 - 100°C
Injection instructions
The material is supplied in airtight bags, ready for use. In case that the virgin material has absorbed moisture, it must be dried with a dehumidified air drying equipment, dew point mini -20°C. Recommended time 2-4hInjection Advice: For reinforced polyamide, Solvay recommends the use of steel with a high content of Carbon and purified for polishing to avoid or limit the abrasion. For example: X38CrMoV5-1 (EN Norm) - 1.2367 /1.2343 (DIN Norm) or X160CrMoV12 (EN Norm) - 1.2601 /1.2379 (DIN Norm). For Mould Temperature, in the case of parts where the surface roughness is required we can recommend a temperature of 90°C to 120°C with an optimum at 105°C. The processing parameters like processing temperatures are a recommendation and can be adjusted in function of injection machine size, part geometry / design
Resin Grade Manufacturer Category Trademark
Royalene® 645 Lion Copolymer, LLC EPDM Royalene®
Sindustris POM N110LDS Sincerity Australia Pty Ltd. Acetal (POM) Homopolymer Sindustris POM
FORMEX® 125BK ITW FORMEX PP, Unspecified FORMEX®
Generic PC - Carbon Powder Generic PC Generic
Axiall PVC 4125-58 Axiall Corporation PVC, Flexible Axiall PVC