Category: | Nylon 6 , Polyamide 6 |
Manufacturer: | Solvay Engineering Plastics |
Trademark: | TECHNYL STAR™ |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | VxCmHZ_TECHNYL-STAR-S-218-V35-BLACK-31-N.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
TECHNYL STAR Polyamide, reinforced with 35% of glass fibre,heat stabilized, for injection moulding. Characterized by a high fluidity of the melt. |
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Appearance |
|
Processing Method |
|
Multi-Point Data |
|
Part Marking Code (ISO 11469) |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.41 | -- | g/cm³ | ISO 1183/A |
Molding Shrinkage | Internal method | |||
Vertical flow direction | 0.53 | -- | % | Internal method |
Flow direction | 0.30 | -- | % | Internal method |
Water Absorption (23°C, 24 hr) | 0.90 | -- | % | ISO 62 |
Molding Shrinkage Isotropy | 0.420 | -- | Internal method |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus | 10700 | 7400 | MPa | ISO 527-2/1A |
Tensile Stress (Break) | 195 | 115 | MPa | ISO 527-2/1A |
Tensile Strain (Break) | 3.0 | 4.5 | % | ISO 527-2/1A |
Flexural Modulus | 10000 | 6200 | MPa | ISO 178 |
Flexural Stress | 295 | 195 | MPa | ISO 178 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength | 13 | 19 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength | 75 | 80 | kJ/m² | ISO 179/1eU |
Notched Izod Impact | 13 | 16 | kJ/m² | ISO 180/1A |
Unnotched Izod Impact Strength | 75 | 80 | kJ/m² | ISO 180 |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 210 | -- | °C | ISO 75-2/Af |
Melting Temperature | 222 | -- | °C | ISO 11357-3 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Flame Rating (1.60 mm) | HB | -- | UL 94 | |
Glow Wire Flammability Index (1.60 mm) | 650 | -- | °C | IEC 60695-2-12 |
Injection | Dry | Unit | |
---|---|---|---|
Drying Temperature | 80.0 | °C | |
Suggested Max Moisture | 0.15 | % | |
Rear Temperature | 220 - 225 | °C | |
Middle Temperature | 225 - 235 | °C | |
Front Temperature | 235 - 245 | °C | |
Mold Temperature | 80.0 | °C |
Injection instructions |
---|
Spiral length vs standard PA: 200% |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 156 LF | RTP Company | PP, Unspecified | RTP |
MOSTEN MA 524 | UNIPETROL RPA | PP Impact Copolymer | MOSTEN |
Grivory® HT2V-3X V0 nat 6059 | EMS-GRIVORY | Nylon 6T/66 | Grivory® |
TOTAL Polyethylene Lumicene® M 4043 UV (EU) | TOTAL Refining & Chemicals | mMDPE | TOTAL Polyethylene |
Sylvin 9077-90LMW Grey 9167 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |