SV-55002U is one of a series of silicone bases Type of HCR designed for applications requiring high strength.
Typical Applications
|
| General Information | |
|---|---|
| Features |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | |
|---|---|---|---|
| Specific Gravity | 1.13 | g/cm³ |
| Hardness | Nominal Value | Unit | |
|---|---|---|---|
| Durometer Hardness | 50 |
| Elastomers | Nominal Value | Unit | |
|---|---|---|---|
| Tensile Strength | 9.31 | MPa | |
| Tensile Elongation (Break) | 660 | % | |
| Tear Strength 1 | 33.3 | kN/m | |
| Compression Set (100°C, 70 hr) | 10 | % |
| Thermoset | Nominal Value | Unit | |
|---|---|---|---|
| Post Cure Time (200°C) | 4.0 | hr |
| Additional Information | Nominal Value | Unit | |
|---|---|---|---|
| Cure Agent | DBPH | ||
| Press / Post Cure: Press |
| Uncured Properties | Nominal Value | Unit | |
|---|---|---|---|
| Curing Time | 0.17 | hr |
| Note Message | |
|---|---|
| 1 . | B mould |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Bergamid™ B70 G10 H BK702 | PolyOne Corporation | Nylon 6 | Bergamid™ |
| ELASTOSIL® R plus 4305/80 | Wacker Chemie AG | Silicone | ELASTOSIL® R plus |
| LNP™ THERMOCOMP™ UF00AAS compound | SABIC Innovative Plastics Europe | PPA | LNP™ THERMOCOMP™ |
| KMI PP KM-S085J | KMI Group, Inc. | PP Random Copolymer | KMI PP |
| Sylvin 6168-80 Grey 9557 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |