| Category: | TPE , Thermoplastic Elastomer |
| Manufacturer: | PolyOne Corporation |
| Trademark: | OnFlex™ |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | Vtr5aV_OnFlex-S-KE-50A-3S1731.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| OnFlex™-S KE thermoplastic elastomer polymer is mixed with hydrogenated styrene block copolymer. This series of polymers has good compatibility and can provide excellent adhesion to a variety of polar substrates, such as PC, ABS, PC/ABS, ASA, and PVC materials. OnFlex-S KE polymer can be processed by 2K molding or multiple injection molding, plug-in molding or co-extrusion. In addition, OnFlex-S KE polymer has good compression set even at high temperatures, good processability, large hardness range, good bending, scratch resistance, colorability, surface appearance, etc. at low temperatures, and excellent mechanical properties. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| RoHS Compliance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.07 | g/cm³ | ISO 1183 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A) | 50 | ISO 868 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ISO 37 | ||
| 100% strain | 1.70 | MPa | ISO 37 |
| 300% strain | 3.90 | MPa | ISO 37 |
| Tensile Stress (Break) | 4.30 | MPa | ISO 37 |
| Tensile Elongation (Break) | 350 | % | ISO 37 |
| Compression Set | ISO 815 | ||
| 23°C, 72 hr | 35 | % | ISO 815 |
| 70°C, 22 hr | 48 | % | ISO 815 |
| 100°C, 22 hr | 68 | % | ISO 815 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Glow Wire Flammability Index (1.00 mm) | 650 | °C | IEC 60695-2-12 |
| Additional Information | Nominal Value | ||
|---|---|---|---|
| General Material Type | Styrene thermoplastic elastomers (TES) | ||
| 各项属性值是采用注射模制基板测量得出。压缩永久变形值是 100°C 时 24 小时零件变形实验得出的值。 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 100 | °C | |
| Drying Time | 2.0 | hr | |
| Processing (Melt) Temp | 200 - 230 | °C | |
| Mold Temperature | 20.0 - 40.0 | °C | |
| Injection Rate | Slow-Moderate |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RAMOFIN PPC301G2 | Polyram Ram-On Industries | PP Copolymer | RAMOFIN |
| Sarlink® TPE ML-1190B BLK X (PRELIMINARY DATA) | Teknor Apex Company | TPE | Sarlink® TPE |
| SUMIPEX® HT03Y | Sumitomo Chemical Co., Ltd. | Acrylic (PMMA) | SUMIPEX® |
| Sylvin 5190-80 Natural | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
| U-polymer UM-8400-20 | UNITIKA Plastics Division | Polyarylate | U-polymer |