Medium Molecular Weight Medium Density Resin Characteristics
Applications
|
General Information | |
---|---|
Additive |
|
Features |
|
Uses |
|
Agency Ratings |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 0.935 | g/cm³ | ASTM D792 |
Melt Mass-Flow Rate (MFR) | ASTM D1238 | ||
190°C/2.16 kg | 0.25 | g/10 min | |
190°C/21.6 kg | 21 | g/10 min |
Films | Nominal Value | Unit | Test Method |
---|---|---|---|
Secant Modulus | ASTM D882 | ||
1% Secant, MD | 441 | MPa | |
1% Secant, TD | 586 | MPa | |
Tensile Strength | ASTM D882 | ||
MD : Yield | 12.4 | MPa | |
TD : Yield | 19.3 | MPa | |
MD : Break | 57.2 | MPa | |
TD : Break | 36.5 | MPa | |
Tensile Elongation | ASTM D882 | ||
MD : Break | 500 | % | |
TD : Break | 900 | % | |
Elmendorf Tear Strength | ASTM D1922 | ||
MD | 18 | g | |
TD | 1400 | g |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Peak Melting Temperature | 126 | °C | ASTM D3417 |
Additional Information | Nominal Value | Unit | Test Method |
---|---|---|---|
Dart Impact | < 50 | g | ASTM D1709 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Melt Temperature | 193 to 216 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Adstif HA5029 | PolyMirae | PP, High Crystal | Adstif |
Ecobarrier® 0914 | Noble Polymers | Polyolefin, Unspecified | Ecobarrier® |
Estane® 2103-80AEF TPU | Lubrizol Advanced Materials, Inc. | TPU-Polyether | Estane® |
Plaslube® POM CO GF30 TL5 | Techmer Engineered Solutions | Acetal (POM) Copolymer | Plaslube® |
POLYfill PPC K20010 | Polykemi AB | PP Copolymer | POLYfill |