tivilon®M 80 Dx 1 is a thermoplastic vulcanized rubber (TPV) product,. It can be processed by extrusion or injection molding and is available in Europe. tivilon®The application areas of M 80 Dx 1 include engineering/industrial accessories and sealing applications. Features include:
|
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Appearance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 0.970 | g/cm³ | ASTM D792 |
| Melt Mass-Flow Rate (MFR) (190°C/5.0 kg) | 4.0 | g/10 min | ASTM D1238 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A, 15 sec) | 80 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength | ASTM D638 | ||
| -- | 10.0 | MPa | ASTM D638 |
| 100% strain | 3.00 | MPa | ASTM D638 |
| 300% strain | 3.80 | MPa | ASTM D638 |
| Tensile Elongation (Break) | 750 | % | ASTM D638 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tear Strength 1 | 42000 | kN/m | ASTM D624 |
| Compression Set (70°C, 24 hr) | 45 | % | ASTM D395 |
| Additional Information |
|---|
| Dx = UV Resistance Level DE = standard UV resistance level DI = medium UV resistance level DR = high UV resistance level |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 75 - 80 | °C | |
| Drying Time | 1.5 - 2.0 | hr | |
| Rear Temperature | 170 - 180 | °C | |
| Middle Temperature | 180 - 190 | °C | |
| Front Temperature | 185 - 200 | °C | |
| Nozzle Temperature | 190 - 210 | °C | |
| Mold Temperature | 35 - 50 | °C | |
| Injection Rate | Moderate-Fast |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 75 - 80 | °C | |
| Drying Time | 1.5 - 2.0 | hr | |
| Cylinder Zone 1 Temp. | 160 - 170 | °C | |
| Cylinder Zone 2 Temp. | 170 - 180 | °C | |
| Cylinder Zone 3 Temp. | 175 - 185 | °C | |
| Cylinder Zone 4 Temp. | 180 - 190 | °C | |
| Die Temperature | 190 - 200 | °C |
| Extrusion instructions |
|---|
| L/D Ratio: >20:1Compression Ratio: 1:2.5 |
| Note Message | |
|---|---|
| 1 . | With Notch |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 283 FR HS | RTP Company | Nylon 66 | RTP |
| Stanyl® TE351 | DSM Engineering Plastics | Nylon 46 | Stanyl® |
| Zytel® RS LC2600 BK043A | DuPont Performance Polymers | Nylon, Unspecified | Zytel® RS |
| NEFTEKHIM PP 8540N (EPF31H) | Nizhnekamskneftekhim Inc. | PP Copolymer | NEFTEKHIM PP |
| HFFR 2003 | Teknor Apex Company | Polyolefin, Unspecified | HFFR |