| Category: | Nylon 612 , Polyamide 612 |
| Manufacturer: | Arkema |
| Trademark: | Hiprolon® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | ViuQbK_Hiprolon-90-VN-LM.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Hiprolon ® 90 VN LM is a polyamide 6.12 neat resin. MAIN APPLICATIONS
|
| General Information | |
|---|---|
| Uses |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.06 | g/cm³ | ISO 1183 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 1700 | MPa | ISO 527-2 |
| Tensile Stress (Yield) | 54.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | > 50 | % | ISO 527-2 |
| Flexural Modulus | 1800 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179 | ||
| -30°C | 7.0 | kJ/m² | |
| 23°C | 10 | kJ/m² | |
| Charpy Unnotched Impact Strength | ISO 179 | ||
| -30°C | No Break | ||
| 23°C | No Break |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Melting Temperature | 215 | °C | ISO 11357-3 |
| Additional Information | Nominal Value | Test Method | |
|---|---|---|---|
| ISO Shortname | PA 612, 27-020 | ISO 1874 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 80.0 to 90.0 | °C | |
| Drying Time | 4.0 | hr | |
| Processing (Melt) Temp | 250 to 290 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Maxelast® F02-087B | Nantong Polymax Elastomer Technology, Co., Ltd | TPE | Maxelast® |
| Stanyl® ForTii™ TX1 | DSM Engineering Plastics | Nylon 4T | Stanyl® ForTii™ |
| Bayfit® 49BM02(90 Index, 70 kg/m³) | Covestro - PUR | PUR, Unspecified | Bayfit® |
| Dryflex® T40 | ELASTO | TPE | Dryflex® |
| Lupoy® GP1000MD | LG Chem Ltd. | PC | Lupoy® |