Category: | PPA , HIGH PERFORMANCE POLYAMIDE RESIN |
Manufacturer: | DuPont Performance Polymers |
Trademark: | Zytel® HTN |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | VAgYQv_Zytel-HTN-FE8200-BK431.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Unreinforced, Toughened, PPA, High Performance Polyamide |
General Information | |
---|---|
Additive |
|
Features |
|
Processing Method |
|
Part Marking Code (ISO 11469) |
|
Part Marking Code (SAE J1344) |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.13 | g/cm³ | ISO 1183 |
Molding Shrinkage | ISO 294-4 | ||
Across Flow | 1.0 | % | |
Flow | 1.0 | % |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 2150 | MPa | ISO 527-2 |
Tensile Stress (Yield) | 69.0 | MPa | ISO 527-2 |
Tensile Strain (Yield) | 5.5 | % | ISO 527-2 |
Nominal Tensile Strain at Break | 14 | % | ISO 527-2 |
Flexural Modulus | 2070 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength (23°C) | 80 | kJ/m² | ISO 179/1eA |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 125 | °C | ISO 75-2/A |
Melting Temperature 1 | 300 | °C | ISO 11357-3 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Volume Resistivity | > 1.0E+15 | ohms·cm | IEC 60093 |
Note Message | |
---|---|
1 . | First Heat |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
REDI-LINK™ DFDA-5440 NT | The Dow Chemical Company | PE, Unspecified | REDI-LINK™ |
SMOKEGUARD™ III 1021 NATURAL UV-FG | AlphaGary | PVC, Unspecified | SMOKEGUARD™ III |
Zetpol® 1000L | Zeon Chemicals L.P. | NBR | Zetpol® |
Dow ENDURANCE™ HFDA-0581 BK | The Dow Chemical Company | TP, Unspecified | Dow ENDURANCE™ |
Wanthane® WHT-8885 | Wanhua Chemical Group Co., Ltd. | TPU-Polyether | Wanthane® |