| Category: | LLDPE , Linear Low Density Polyethylene |
| Manufacturer: | HANWHA TOTAL PETROCHEMICALS Co., Ltd. |
| Trademark: | Hanwha Total PE |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | V3Dfb3_Hanwha-Total-PE-4220F.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Hanwha Total PE 4220F is a linear low density polyethylene product,. It can be processed by blowing film and is available in North America or Asia Pacific. The application areas of Hanwha Total PE 4220F include bags/linings and packaging. Features include:
|
| General Information | |
|---|---|
| Additive |
|
| Features |
|
| Uses |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.921 | g/cm³ | ASTM D1505 |
| Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 0.90 | g/10 min | ASTM D1238 |
| Films | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Film Thickness - Tested | 38 | µm | |
| Tensile Strength | ASTM D882 | ||
| MD : Yield, 38 µm | 9.81 | MPa | ASTM D882 |
| TD : Yield, 38 µm | 10.8 | MPa | ASTM D882 |
| MD : Fracture, 38 µm | 40.2 | MPa | ASTM D882 |
| TD : Fracture, 38 µm | 31.4 | MPa | ASTM D882 |
| Tensile Elongation | ASTM D882 | ||
| MD : Fracture, 38 µm | 620 | % | ASTM D882 |
| TD : Fracture, 38 µm | 840 | % | ASTM D882 |
| Elmendorf Tear Strength | ASTM D1922 | ||
| MD : 25 µm | 150 | g | ASTM D1922 |
| TD : 25 µm | 370 | g | ASTM D1922 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Brittleness Temperature | -70.0 | °C | ASTM D746 |
| Vicat Softening Temperature | 100 | °C | ASTM D1525 |
| Optical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Gloss (45°, 38.0 µm) | 55 | ASTM D2457 | |
| Haze (38.0 µm) | 11 | % | ASTM D1003 |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Cylinder Zone 1 Temp. | 170 - 190 | °C | |
| Cylinder Zone 2 Temp. | 170 - 190 | °C | |
| Cylinder Zone 3 Temp. | 170 - 190 | °C | |
| Cylinder Zone 4 Temp. | 170 - 190 | °C | |
| Cylinder Zone 5 Temp. | 170 - 190 | °C | |
| Die Temperature | 190 - 200 | °C |
| Extrusion instructions |
|---|
| Blow up ratio: 1.0 to 2.0 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| MBA PP 2123 | MBA Polymers | PP Copolymer | MBA PP |
| Sylvin 9639-83AM Clear 8354 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
| ALAMID® 6.6 GK 30 | LEIS Polytechnik - polymere Werkstoffe GmbH | Nylon 66 | ALAMID® |
| Celstran® PP-GF50-02- Natural | Celanese Corporation | PP, Unspecified | Celstran® |
| CYCOLOY™ CM6210 resin | SABIC Innovative Plastics | PC+ABS | CYCOLOY™ |