| Category: | PBT , Polybutylene Terephthalate |
| Manufacturer: | Polyplastics Co., Ltd. |
| Trademark: | DURANEX® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | UaSg91_DURANEXCN7000LNLB.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
DURANEX®CN7000LN/LB is a polybutene terephthalate (PBT) product,. It can be processed by injection molding and is available in North America, Europe or the Asia-Pacific region. Features include:
|
| General Information | |
|---|---|
| Additive |
|
| Features |
|
| UL File Number |
|
| Forms |
|
| Processing Method |
|
| Part Marking Code (ISO 11469) |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.42 | g/cm³ | ISO 1183 |
| Water Absorption (23°C, 24 hr) | 0.20 | % | ISO 62 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Rockwell Hardness (M-Scale) | 80 | ISO 2039-2 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | 54.0 | MPa | ISO 527-2 |
| Nominal Tensile Strain at Break | 11 | % | ISO 527-2 |
| Flexural Modulus | 2310 | MPa | ISO 178 |
| Flexural Stress | 81.0 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength (23°C) | 3.3 | kJ/m² | ISO 179/1eA |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 64.0 | °C | ISO 75-2/A |
| Linear thermal expansion coefficient | Internal method | ||
| Flow : 23 to 55°C | 1.0E-4 | cm/cm/°C | Internal method |
| Lateral : 23 to 55°C | 1.0E-4 | cm/cm/°C | Internal method |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Volume Resistivity | 6.0E+15 | ohms·cm | IEC 60093 |
| Dielectric Strength (3.00 mm) | 17 | kV/mm | IEC 60243-1 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flame Rating | V-0 | UL 94 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 120 - 140 | °C | |
| Drying Time | 3.0 - 5.0 | hr | |
| Rear Temperature | 250 - 270 | °C | |
| Middle Temperature | 250 - 270 | °C | |
| Front Temperature | 250 - 270 | °C | |
| Mold Temperature | 40 - 80 | °C | |
| Holding Pressure | 60.0 - 100 | MPa | |
| Screw Speed | 100 - 150 | rpm |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 600 TFE 10 FR | RTP Company | ABS | RTP |
| Grilamid® 2S 25 W 20 X nat | EMS-GRIVORY | Nylon 610 | Grilamid® |
| Osterlene® PPC-57-1.4-N | Osterman & Company | PP Impact Copolymer | Osterlene® |
| apigo bio® PM 900 | API SpA | TPO (POE) | apigo bio® |
| LNP™ LUBRICOMP™ Cycoloy_C2801 compound | SABIC Innovative Plastics | PC+ABS | LNP™ LUBRICOMP™ |