| Category: | Nylon 66/6 , Polyamide 66/6 Copolymer |
| Manufacturer: | Wellman Engineering Resins |
| Trademark: | Wellamid® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | ULgf30_Wellamid-GF33-66-6-XE-BK167A.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Wellamid® GF33-66/6 XE-BK167A is a Polyamide 66/6 Copolymer (Nylon 66/6) material filled with 33% glass fiber. It is available in Asia Pacific, Europe, Latin America, or North America. |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.42 | g/cm³ | ISO 1183 |
| Molding Shrinkage | ISO 294-4 | ||
| Across Flow : 23°C | 0.90 to 1.3 | % | |
| Flow : 23°C | 0.20 to 0.60 | % |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Yield, 23°C) | 145 | MPa | ISO 527-2 |
| Tensile Strain (Yield, 23°C) | 2.0 | % | ISO 527-2 |
| Flexural Modulus (23°C) | 9000 | MPa | ISO 178 |
| Flexural Stress (23°C) | 210 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength (23°C) | 5.0 | kJ/m² | ISO 180 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 220 | °C | ISO 75-2/A |
| Melting Temperature (DSC) | 260 | °C | ISO 3146 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Badamid® LB70 K | Bada AG | Nylon 6 | Badamid® |
| Jampilen EP300D | Jam Polypropylene Company | PP Copolymer | Jampilen |
| Plaskon MUF-2C | Cookson Electronics - Semiconductor Products | Epoxy | Plaskon |
| Plaslube® POM CO UV BK | Techmer Engineered Solutions | Acetal (POM) Copolymer | Plaslube® |
| PlexTuf L-66119 | Altuglas International of Arkema Inc. | Acrylic (PMMA) | PlexTuf |