Category: | TPO (POE) , Thermoplastic Polyolefin Elastomer |
Manufacturer: | R&P (Pte.) Ltd. |
Trademark: | STERLENE™ |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | U2hVIB_STERLENE-CMV208.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
STERLENE™ CMV208 is a compound with high stiffness and medium impact designed for automotive interior trim application. |
General Information | |
---|---|
Features |
|
Uses |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.03 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) 1(230°C/2.16 kg) | 16 | g/10 min | ISO 1133 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus (23°C) | 2740 | MPa | ISO 527-2/50 |
Tensile Stress (Yield, 23°C) | 27.0 | MPa | ISO 527-2/50 |
Tensile Strain | ISO 527-2/50 | ||
Yield, 23°C | 5.2 | % | |
Break, 23°C | 23 | % | |
Flexural Modulus 2(23°C) | 2390 | MPa | ISO 178 |
Flexural Stress 3(23°C) | 39.0 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact Strength (23°C, Complete Break) | 9.5 | kJ/m² | ISO 180/A |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 58.0 | °C | ISO 75-2/Af |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Time | 2.0 | hr | |
Processing (Melt) Temp | 190 to 240 | °C | |
Mold Temperature | 25.0 to 60.0 | °C |
Note Message | |
---|---|
1 . | Procedure B |
2 . | 2.0 mm/min |
3 . | 2.0 mm/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Topilene® J740 | Hyosung Corporation | PP Impact Copolymer | Topilene® |
ALCUDIA® EVA PA-411 | REPSOL | EVA | ALCUDIA® EVA |
PLUSTEK PA301G6 | Polyram Ram-On Industries | Nylon 66 | PLUSTEK |
LNP™ THERMOCOMP™ 5C004 compound | SABIC Innovative Plastics | PVDF | LNP™ THERMOCOMP™ |
LNP™ STAT-KON™ AE004 compound | SABIC Innovative Plastics | ABS | LNP™ STAT-KON™ |