| Category: | PP Homopolymer , Polypropylene Homopolymer |
| Manufacturer: | ALBIS PLASTIC GmbH |
| Trademark: | ALTECH® PP-H |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | TxyM4s_ALTECHPPHA2050500GF50.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
ALTECH®PP-H A 2050/500 GF50 is a polypropylene homopolymer (PP Homopoly) product, and the filler is 50% glass fiber reinforced material. It can be processed by injection molding and is available in North America, Europe or the Asia-Pacific region. Typical application areas are: architectural applications. Features include:
|
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Features |
|
| Uses |
|
| Agency Ratings |
|
| RoHS Compliance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.32 | g/cm³ | ISO 1183 |
| Melt Volume-Flow Rate (MVR) (230°C/2.16 kg) | 2.00 | cm³/10min | ISO 1133 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 9000 | MPa | ISO 527-2 |
| Tensile Stress | 55.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 1.0 | % | ISO 527-2 |
| Flexural Modulus | 8600 | MPa | ISO 178 |
| Flexural Stress | 80.0 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179/1eA | ||
| -- | 7.0 | kJ/m² | ISO 179/1eA |
| -40°C | 5.0 | kJ/m² | ISO 179/1eA |
| Charpy Unnotched Impact Strength | ISO 179/1eU | ||
| -- | 11 | kJ/m² | ISO 179/1eU |
| -40°C | 11 | kJ/m² | ISO 179/1eU |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 140 | °C | ISO 75-2/A |
| Vicat Softening Temperature | 112 | °C | ISO 306/B50 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | |||
| Dehumidification desiccant | 80 - 120 | °C | |
| Hot air dryer | 80 - 120 | °C | |
| Drying Time | |||
| Dehumidification desiccant | 2.0 - 4.0 | hr | |
| Hot air dryer | 2.0 - 3.0 | hr | |
| Processing (Melt) Temp | 200 - 270 | °C | |
| Mold Temperature | 20 - 90 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Sarlink® TPV 3139DN | Teknor Apex Company | TPV | Sarlink® TPV |
| SLOVAMID® 6 GF 15 T 25 | Plastcom | Nylon 6 | SLOVAMID® 6 |
| Witcom PA6 5G-AS-S | Witcom Engineering Plastics B.V. | Nylon 6 | Witcom PA6 |
| ALCUDIA® LDPE PE-034 | REPSOL | LDPE | ALCUDIA® LDPE |
| Cellophane™ 340XSB | Innovia Films Ltd. | Cellulose, Regenerated | Cellophane™ |