DILAMID® 6 FV 15 NATURAL

Category: Nylon 6 , Polyamide 6
Manufacturer: Dilaplast S.p.A.
Trademark: DILAMID®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: TvfbCM_DILAMID-6-FV-15-NATURAL.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
DILAMID® 6 FV 15 NATURAL is a Polyamide 6 (Nylon 6) material filled with 15% glass fiber. It is available in Europe for injection molding.
General Information
Filler / Reinforcement
  • Glass Fiber, 15% Filler by Weight
Appearance
  • Natural Color
Forms
  • Pellets
Processing Method
  • Injection Molding
PhysicalNominal ValueUnitTest Method
Density 1.23g/cm³ISO 1183
Molding Shrinkage - Flow 0.50 to 0.70%ASTM D955
MechanicalNominal ValueUnitTest Method
Tensile Stress (Yield)120MPaISO 527-2
Tensile Strain (Break)4.0%ISO 527-2
Flexural Modulus 4.50MPaISO 178
ImpactNominal ValueUnitTest Method
Notched Izod Impact Strength (23°C)7.0kJ/m²ISO 180
ThermalNominal ValueUnitTest Method
Heat Deflection Temperature (1.8 MPa, Unannealed)200°CISO 75-2/A
Vicat Softening Temperature 210°CISO 306/B50
ElectricalNominal ValueUnitTest Method
Dielectric Strength 21kV/mmASTM D149
Comparative Tracking Index 500VIEC 60112
FlammabilityNominal ValueUnitTest Method
Glow Wire Ignition Temperature (2.00 mm)650°CIEC 60695-2-13
InjectionNominal ValueUnit
Drying Temperature 70.0 to 90.0°C
Drying Time 2.0 to 8.0hr
Suggested Max Moisture 0.20%
Rear Temperature 240 to 280°C
Middle Temperature 250 to 290°C
Front Temperature 260 to 300°C
Nozzle Temperature 255 to 295°C
Processing (Melt) Temp 260 to 300°C
Mold Temperature 70.0 to 110°C
Resin Grade Manufacturer Category Trademark
Bayblend® FR3040 Covestro - Polycarbonates PC+ABS Bayblend®
FLEXITEQ™ F75A110 Marplex Australia Pty. Ltd. TPV FLEXITEQ™
EOS PA 2200 Speed 1.0 EOS GmbH Nylon 12 EOS
POFEX 8200EP80F POLYROCKS CHEMICAL CO., LTD TPE POFEX
ESTOPLAST EP 4020WW26 Ester Industries Ltd. PBT ESTOPLAST EP