Sarlink®TPE EE-2245N is a thermoplastic elastomer (TPE) material,. This product is available in North America, Africa and the Middle East, Latin America, Europe or Asia Pacific. The processing method is: extrusion. Sarlink®The typical application field of TPE EE-2245N is: automobile industry |
General Information | |
---|---|
Uses |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.17 | g/cm³ | ASTM D792 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 0.20 | g/10 min | ASTM D1238 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness | ASTM D2240 | ||
Shaw A | 48 | ASTM D2240 | |
Shaw A, 15 seconds | 45 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | ASTM D412 | ||
Transverse flow : 100% strain | 0.965 | MPa | ASTM D412 |
Flow : 100% strain | 1.45 | MPa | ASTM D412 |
Tensile Strength | ASTM D412 | ||
Transverse flow : Fracture | 6.34 | MPa | ASTM D412 |
Flow : Fracture | 4.07 | MPa | ASTM D412 |
Tensile Elongation | ASTM D412 | ||
Transverse flow : Fracture | 890 | % | ASTM D412 |
Flow : Fracture | 700 | % | ASTM D412 |
Compression Set | ASTM D395 | ||
23°C, 22 hr | 13 | % | ASTM D395 |
70°C, 22 hr | 28 | % | ASTM D395 |
125°C, 70 hr | 77 | % | ASTM D395 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Rear Temperature | 199 - 210 | °C | |
Middle Temperature | 204 - 216 | °C | |
Front Temperature | 210 - 221 | °C | |
Nozzle Temperature | 216 - 227 | °C | |
Processing (Melt) Temp | 216 - 227 | °C | |
Mold Temperature | 35.0 - 65.6 | °C | |
Injection Pressure | 1.38 - 6.89 | MPa | |
Injection Rate | Fast | ||
Back Pressure | 0.172 - 0.862 | MPa | |
Screw Speed | 50 - 120 | rpm | |
Cushion | 3.81 - 25.4 | mm |
Injection instructions |
---|
无需干燥。但如果湿度过大,则将粒料在150°F (65°C)的温度下干燥2-4小时。 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Cylinder Zone 1 Temp. | 193 - 204 | °C | |
Cylinder Zone 2 Temp. | 199 - 210 | °C | |
Cylinder Zone 3 Temp. | 204 - 216 | °C | |
Cylinder Zone 5 Temp. | 210 - 221 | °C | |
Die Temperature | 216 - 227 | °C |
Extrusion instructions |
---|
螺杆转速30 - 100 rpm |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Vibrathane® B629 | Chemtura | PUR-Ether/TDI | Vibrathane® |
TRILOY® MH275M | Samyang Corporation | PC+ABS | TRILOY® |
Niplene C40 | Soredi S.p.a. | PP Homopolymer | Niplene |
4MID® 9A22325 | 4Plas | Nylon 66 | 4MID® |
Ad-Tech Epoxy ES-216-AC | Ad-Tech Plastic Systems Corp. | Epoxy | Ad-Tech Epoxy |