| Category: | TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester) |
| Manufacturer: | COIM S.p.A. |
| Trademark: | LARIPUR® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | Sok88m_LARIPUR-LPR-8020.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
LARIPUR®LPR 8020 is a thermoplastic polyurethane elastomer (polyester)(TPU-polyester) material,. This product is available in North America, Latin America or Europe. The processing method is injection molding. LARIPUR®The main features of LPR 8020 are:
|
| General Information | |
|---|---|
| Features |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.21 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A) | 82 | ASTM D2240 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ASTM D412 | ||
| 50% strain | 3.80 | MPa | ASTM D412 |
| 100% strain | 5.30 | MPa | ASTM D412 |
| 300% strain | 10.2 | MPa | ASTM D412 |
| Tensile Strength (Break) | 48.2 | MPa | ASTM D412 |
| Tensile Elongation (Break) | 590 | % | ASTM D412 |
| Tear Strength | 78.0 | kN/m | ASTM D624 |
| Compression Set | ASTM D395 | ||
| 23°C, 70 hr | 18 | % | ASTM D395 |
| 70°C, 22 hr | 41 | % | ASTM D395 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Vicat Softening Temperature | 84.0 | °C | ASTM D1525 |
| Additional Information |
|---|
| Abrasion loss, DIN 53516: 30mm³ |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 200 H Z | RTP Company | Nylon 66 | RTP |
| Spectar™ FR1000 | Eastman Chemical Company | Copolyester | Spectar™ |
| Flexirene® MS 40 DA | Versalis S.p.A. | LLDPE | Flexirene® |
| Hifax SP 1079/94 | LyondellBasell Industries | PP Copolymer | Hifax |
| Sylvin 5132-75 Clear Blue 8372 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |