Category: | TPV , Thermoplastic Vulcanizate |
Manufacturer: | Salflex Polymers Ltd. |
Trademark: | Salflex |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | SkHGLV_Salflex-364A.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Salflex 364A is a thermoplastic vulcanized rubber (TPV) product,. It can be processed by blow molding, extrusion or injection molding, and is available in North America. The application areas of Salflex 364A include the automotive industry and bags/linings. Features include:
|
General Information | |
---|---|
Features |
|
Uses |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 0.950 | g/cm³ | ASTM D792 |
Molding Shrinkage - Flow | 1.5 | % | ASTM D955 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A, 5 sec) | 63 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (100% Strain) | 2.40 | MPa | ASTM D412 |
Tensile Strength (Break) | 5.80 | MPa | ASTM D412 |
Tensile Elongation (Break) | 400 | % | ASTM D412 |
Tear Strength | 33.0 | kN/m | ASTM D624 |
Compression Set (70°C, 22 hr) | 45 | % | ASTM D395 |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Change in Tensile Strength in Air (150°C, 168 hr) | -12 | % | ASTM D573 |
Change in Ultimate Elongation in Air (150°C, 168 hr) | 28 | % | ASTM D573 |
Change in Durometer Hardness in Air (Shore A, 150°C, 168 hr) | -4.0 | ASTM D573 | |
Change in Tensile Strength (125°C, 70 hr, in IRM 903 Oil) | -34 | % | ASTM D471 |
Change in Ultimate Elongation (125°C, 70 hr, in IRM 903 Oil) | -19 | % | ASTM D471 |
Change in Volume (125°C, 70 hr, ASTM Standard Oil (No.3)) | 88 | % | ASTM D471 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Brittleness Temperature | -60.0 | °C | ASTM D746 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 60.0 - 75.0 | °C | |
Drying Time | 2.0 - 4.0 | hr | |
Cylinder Zone 1 Temp. | 175 - 205 | °C | |
Cylinder Zone 2 Temp. | 175 - 210 | °C | |
Cylinder Zone 3 Temp. | 175 - 210 | °C | |
Cylinder Zone 4 Temp. | 175 - 220 | °C | |
Melt Temperature | 180 - 210 | °C | |
Die Temperature | 175 - 215 | °C |
Extrusion instructions |
---|
Blow Molding Mold Temperature: 5 to 60°C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Sasol Polymers PP CPV340 | Sasol Polymers | PP Impact Copolymer | Sasol Polymers PP |
Boda BDT2461E | Chenguang Fluoro & Silicone Elastomers Co., Ltd. | Fluorelastomer | Boda |
HiFill® PA6 0177 B | Techmer Engineered Solutions | Nylon 6 | HiFill® |
KumhoSunny PC HCG2520MP | Shanghai KumhoSunny Plastics Co., Ltd. | PC | KumhoSunny PC |
POLYblend PC/ABS 45V | Polykemi AB | PC+ABS | POLYblend |