Category: | TPE , Thermoplastic Elastomer |
Manufacturer: | Shanghai Lin Gen Rubber Materials Co., Ltd. |
Trademark: | Delene |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | SHrXsD_Delene5590.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Halogen free flame retardant TPE for Wire & Cable applications, with excellent elasticity |
General Information | |
---|---|
Features |
|
Uses |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.07 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness | ASTM D2240 | ||
Shaw A | 90 | ASTM D2240 | |
Shaw D | 35 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength (Yield) | 10.0 | MPa | ASTM D412 |
Tensile Elongation (Break) | 450 | % | ASTM D412 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Volume Resistivity | > 1.0E+14 | ohms·cm | ASTM D257 |
Dielectric Strength | > 20 | kV/mm | ASTM D149 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating (3.0 mm) | V-0 | UL 94 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 80 - 90 | °C | |
Drying Time | 3.0 - 4.0 | hr |
Extrusion instructions |
---|
Hopper Temperature: 150 - 170 °CTransmission Temperature: 180 - 200 °CMeasurement Temperature: 200 - 230 °CDie Temperature: 190 - 220 °CMesh Temperature: 100 - 200 mesh |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
SAXALEN™ PPH325GK20 | SAX Polymers | PP Homopolymer | SAXALEN™ |
NEALID XN013C - 8428 | AD majoris | Nylon, Unspecified | NEALID |
ELASTOSIL® E 60 | Wacker Chemie AG | Silicone | ELASTOSIL® E |
Generic PP Homopolymer - Glass\Mineral | Generic | PP Homopolymer | Generic |
Hifax CA 1110 G4 LS C12477 | LyondellBasell Industries | PP Copolymer | Hifax |