| Category: | TPE , Thermoplastic Elastomer |
| Manufacturer: | Elastocon TPE Technologies |
| Trademark: | Elastocon® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | SGbSep_Elastocon2840FX.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Elastocon® 2840FX is a functionalized translucent thermoplastic elastomer compound formulated for applications that require rubber-like properties and high resilience. Elastocon® 2840FX is well suited for consumer goods and industrial applications requiring U.V. stability. Elastocon 2840FX has been developed for applications requiring print ability and overmolding onto various metals and other non-plastic substrates. Elastocon® 2840FX is supplied as ready to use pellets in 50 lb. quantities. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 0.920 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A) | 40 | ASTM D2240 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (100% Strain) | 1.20 | MPa | ASTM D412 |
| Tensile Strength | 4.50 | MPa | ASTM D412 |
| Tensile Elongation (Break) | 320 | % | ASTM D412 |
| Tear Strength | 15.4 | kN/m | ASTM D624 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Rear Temperature | 177 | °C | |
| Middle Temperature | 188 - 199 | °C | |
| Front Temperature | 193 - 204 | °C | |
| Nozzle Temperature | 199 - 204 | °C | |
| Processing (Melt) Temp | 199 - 204 | °C | |
| Mold Temperature | 38 - 49 | °C | |
| Injection Rate | Slow-Moderate | ||
| Back Pressure | 0.345 - 1.03 | MPa |
| Injection instructions |
|---|
| Elastocon® 2840FX thermoplastic elastomer compound does not require drying. |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Cylinder Zone 1 Temp. | 154 - 160 | °C | |
| Cylinder Zone 2 Temp. | 160 - 171 | °C | |
| Cylinder Zone 3 Temp. | 171 - 177 | °C | |
| Cylinder Zone 4 Temp. | 182 - 188 | °C | |
| Cylinder Zone 5 Temp. | 177 - 182 | °C | |
| Die Temperature | 160 - 171 | °C |
| Extrusion instructions |
|---|
| Screw Speed: 75 to 125 RPM |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| SCANAMID 6 B11^ F30 FR5 | Polykemi AB | Nylon 6 | SCANAMID 6 |
| SLOVASTER® B BT | Plastcom | PBT | SLOVASTER® |
| Cri-Line LC-715 | Cri-Tech, Inc. | Fluorelastomer | Cri-Line |
| KumhoSunny ASA XC811 | Shanghai KumhoSunny Plastics Co., Ltd. | ASA | KumhoSunny ASA |
| Karina IVORY PVC COMPOUND 105951-35/1-A-AC | Karina Ind. e Com. de Plásticos Ltda | PVC, Unspecified | Karina |