Category: | TPV , Thermoplastic Vulcanizate |
Manufacturer: | RTP Company |
Trademark: | RTP |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | SGRiyb_RTP-2800-B-65A-FR-A.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Flame Retardant - PBDE Free |
General Information | |
---|---|
Features |
|
RoHS Compliance |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.25 | g/cm³ | ASTM D792 |
Moisture Content | 0.030 | % |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A, 10 sec) | 65 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress 1(100% Strain, 3.18 mm) | 2.28 | MPa | ASTM D412 |
Tensile Strength 2(Yield, 3.20 mm) | 4.48 | MPa | ASTM D412 |
Tensile Elongation 3(Break) | 500 | % | ASTM D412 |
Tear Strength 4 | 21.9 | kN/m | ASTM D624 |
Compression Set 5 | ASTM D395B | ||
23°C, 22 hr | 24 | % | |
70°C, 22 hr | 39 | % |
Flammability | Nominal Value | Test Method | |
---|---|---|---|
Flame Rating (1.50 mm) | V-0 | UL 94 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 79.4 | °C | |
Drying Time | 2.0 | hr | |
Dew Point | -17.8 | °C | |
Processing (Melt) Temp | 182 to 210 | °C | |
Mold Temperature | 15.6 to 65.6 | °C | |
Injection Pressure | 82.7 to 124 | MPa |
Note Message | |
---|---|
1 . | Die C, 510 mm/min |
2 . | Die C, 500 mm/min |
3 . | Die C, 500 mm/min |
4 . | Die C |
5 . | Type 2 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Tecotek® BC40 UF65 NL CE | Eurotec Engineering Plastics | PC+ABS | Tecotek® |
SLOVASTER® B1 BT TS | Plastcom | PBT | SLOVASTER® |
POLYfill PP HBK30030 | Polykemi AB | PP Homopolymer | POLYfill |
SCHULAMID® 612 GF 33 HE | A. Schulman Europe | Nylon 612 | SCHULAMID® |
Edgetek™ ET2020-0001 FR | PolyOne Corporation | Copolyester | Edgetek™ |