| Category: | PESU , Polyethersulfone |
| Manufacturer: | RTP Company |
| Trademark: | RTP |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | S47lxg_RTP-1400-GB-30.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Glass Bead |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| RoHS Compliance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.56 | g/cm³ | ASTM D792 |
| Molding Shrinkage - Flow (3.20 mm) | 0.80 | % | ASTM D955 |
| Moisture Content | 0.040 | % |
| Additional Information | Nominal Value | Unit | |
|---|---|---|---|
| Primary Additive | 30 | % |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 4140 | MPa | ASTM D638 |
| Tensile Strength | 68.9 | MPa | ASTM D638 |
| Tensile Elongation (Yield) | 2.5 | % | ASTM D638 |
| Flexural Modulus | 4140 | MPa | ASTM D790 |
| Flexural Strength | 117 | MPa | ASTM D790 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact (3.20 mm) | 43 | J/m | ASTM D256 |
| Unnotched Izod Impact (3.20 mm) | 290 | J/m | ASTM D4812 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 149 | °C | |
| Drying Time | 6.0 | hr | |
| Dew Point | -31.7 | °C | |
| Processing (Melt) Temp | 343 - 377 | °C | |
| Mold Temperature | 135 - 177 | °C | |
| Injection Pressure | 68.9 - 103 | MPa |
| Injection instructions |
|---|
| Desiccant Type Dryer Required. |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| SABIC® PP RA12MN40 | Saudi Basic Industries Corporation (SABIC) | PP Random Copolymer | SABIC® PP |
| Terluran® GP-25 | INEOS Styrolution Group GmbH | ABS | Terluran® |
| MAJORIS G474 | AD majoris | PP, Unspecified | MAJORIS |
| KMI PP KM-085IB | KMI Group, Inc. | PP Impact Copolymer | KMI PP |
| ULTEM™ AUT195 resin | SABIC Innovative Plastics | PEI+PCE | ULTEM™ |