Category: | Nylon 66 , Polyamide 66 |
Manufacturer: | Teknor Apex Company (Chem Polymer) |
Trademark: | Chemlon® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | S18irQ_Chemlon-135-GH.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Chemlon® 135 GH is a Polyamide 66 (Nylon 66) material filled with glass fiber. It is available in Asia Pacific, Europe, or North America for injection molding. Primary attribute of Chemlon® 135 GH: Flame Rated. Typical application of Chemlon® 135 GH: Automotive |
General Information | |
---|---|
Filler / Reinforcement |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.40 | g/cm³ | ASTM D792 |
Molding Shrinkage - Flow | 0.15 to 0.30 | % | ASTM D955 |
Water Absorption (24 hr) | 0.85 | % | ASTM D570 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | 193 | MPa | ASTM D638 |
Tensile Elongation | ASTM D638 | ||
Yield | 3.0 | % | |
Break | 3.0 | % | |
Flexural Modulus | 9140 | MPa | ASTM D790 |
Flexural Strength | 276 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (23°C) | 110 | J/m | ASTM D256 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Deflection Temperature Under Load (1.8 MPa, Unannealed) | 253 | °C | ASTM D648 |
Melting Temperature | 257 | °C | |
CLTE - Flow | 5.0E-5 | cm/cm/°C | ASTM D696 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Volume Resistivity | 1.0E+14 | ohms·cm | ASTM D257 |
Dielectric Strength (3.00 mm) | 16 | kV/mm | ASTM D149 |
Dielectric Constant (1 MHz) | 3.90 | ASTM D150 | |
Dissipation Factor (1 MHz) | 0.020 | ASTM D150 | |
Comparative Tracking Index (CTI) | 600 | V | UL 746 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating (0.810 mm) | HB | UL 94 | |
Oxygen Index | 25 | % | ASTM D2863 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 79.4 | °C | |
Suggested Max Moisture | 0.20 | % | |
Suggested Max Regrind | 25 | % | |
Rear Temperature | 246 to 257 | °C | |
Middle Temperature | 263 to 279 | °C | |
Front Temperature | 268 to 285 | °C | |
Nozzle Temperature | 268 to 285 | °C | |
Processing (Melt) Temp | 266 to 282 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Rilsamid® AESNO MED | Arkema | Nylon 12 | Rilsamid® |
RTP 4099 X 112302 | RTP Company | PPA | RTP |
ASI POLYPROPYLENE 3515 | A. Schulman Inc. | PP Copolymer | ASI POLYPROPYLENE |
Latilub 87/24UV-20T | LATI S.p.A. | PC | Latilub |
ULTEM™ 2410 resin | SABIC Innovative Plastics | PEI | ULTEM™ |