| OnFlex™-S HF thermoplastic elastomer polymer is mixed with hydrogenated styrene block copolymer. This series of polymers uses a unique, patent-pending halogen-free flame retardant system. And, OnFlex™-S HF polymer has good mechanical properties, meets the requirements of UL94 V-0, has good oxygen limit index (LOI) value, large hardness range, good processability, and excellent stability to ultraviolet rays. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| RoHS Compliance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.09 | g/cm³ | ISO 1183 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A) | 50 | ISO 868 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ISO 37 | ||
| 100% strain | 1.10 | MPa | ISO 37 |
| 300% strain | 2.00 | MPa | ISO 37 |
| Tensile Stress (Break) | 2.50 | MPa | ISO 37 |
| Tensile Elongation (Break) | 400 | % | ISO 37 |
| Tear Strength | 24 | kN/m | ISO 34-1 |
| Compression Set | ISO 815 | ||
| 23°C, 72 hr | 10 | % | ISO 815 |
| 70°C, 22 hr | 40 | % | ISO 815 |
| 100°C, 22 hr | 77 | % | ISO 815 |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Comparative Tracking Index | 550 | V | IEC 60112 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flame Rating (1.50 mm) | V-0 | UL 94 | |
| Glow Wire Flammability Index (2.00 mm) | 960 | °C | IEC 60695-2-12 |
| Glow Wire Ignition Temperature (2.00 mm) | 725 | °C | IEC 60695-2-13 |
| Oxygen Index | 36 | % | ISO 4589-2 |
| Additional Information | Nominal Value | ||
|---|---|---|---|
| General Material Type | Styrene thermoplastic elastomers (TES) | ||
| 各项属性值是采用注射模制基板测量得出。 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 80.0 | °C | |
| Drying Time | 2.0 | hr | |
| Processing (Melt) Temp | 160 - 180 | °C | |
| Mold Temperature | 30.0 - 50.0 | °C | |
| Injection Rate | Moderate-Fast |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP ESD 2285 HF | RTP Company | PEEK | RTP |
| RheTech Polypropylene FRP256-01 | RheTech, Inc. | PP Copolymer | RheTech Polypropylene |