Advanced Composites ATX832D

Category: TPO , Compounded Polypropylene
Manufacturer: Advanced Composites, Inc.
Trademark: Advanced Composites
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: RwrkAZ_Advanced-Composites-ATX832D.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Advanced Composites ATX832D is a composite polypropylene product, which contains talc filler. It is available in North America. Typical application areas are: automotive industry.

Features include:
  • Impact modification
  • scratch resistance
General Information
Filler / Reinforcement
  • Talc filler
Additive
  • Impact modifier
Features
  • Impact modification
  • Scratch resistance
Forms
  • Particle
PhysicalNominal ValueUnitTest Method
Density 1.03g/cm³ISO 1183
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg)30g/10 minISO 1133
MechanicalNominal ValueUnitTest Method
Tensile Stress (Yield)22.0MPaISO 527-2
Flexural Modulus 1940MPaISO 178
ImpactNominal ValueUnitTest Method
Instrumented Dart Impact 1ASTM D3763
    0°C, Total Energy 23.3JASTM D3763
    23°C, Total Energy 23.6JASTM D3763
InjectionNominal ValueUnit
Drying Temperature 100°C
Drying Time 2.0 - 4.0hr
Rear Temperature 204°C
Middle Temperature 218°C
Front Temperature 218°C
Nozzle Temperature 216°C
Processing (Melt) Temp 204 - 232°C
Mold Temperature 48.9 - 60.0°C
Cushion 6.35 - 12.7mm
Injection instructions
Injection Pressure: 10% over max fill pressureHolding Pressure: 50 to 60% of max fill pressureInjection Speed: 1 to 3 inches/secScrew RPM: 1 to 2 secs before mold open
Note Message
1 .6.60 m/sec
Resin Grade Manufacturer Category Trademark
Melthene® -G Melthene®-G TOSOH Corporation EVA Melthene® -G
SLOVALEN® PH 49 GF 30 TS Plastcom PP, Unspecified SLOVALEN®
SPESIN® KP513MT25BK Kolon Plastics, Inc. PBT SPESIN®
REV Materials 8008-003 REV Materials PP, Unspecified REV Materials
Sarlink® TPE EE-2270B (PRELIMINARY DATA) Teknor Apex Company TPE Sarlink® TPE