Andur 8200 AP/Curene® 442

Category: PUR-Ether/TDI , Polyurethane (Polyether, TDI)
Manufacturer: Anderson Development Company
Trademark: Andur
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: RpNxtf_Andur-8200-AP-Curene-442.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Andur 8200-AP is a polyether (PPG) based liquid, toluene diisocyanate terminated prepolymer. An elastomer with a hardness of 82 to 84 Shore A is obtained when this prepolymer is cured with Curene 442 [4,4'-methylene-bis (orthochloroaniline)]. Elastomers of lower hardness can be obtained by reaction with various polyols and their combination with Curene 442 and other diamines, or through the use of plasticizers.
General Information
Forms
  • Liquid
PhysicalNominal ValueUnitTest Method
Density 1.11g/cm³ASTM D1505
Molding Shrinkage - Flow 1.5%ASTM D955
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shore A)83ASTM D2240
ElastomersNominal ValueUnitTest Method
Tensile Stress ASTM D412
    100% strain 4.48MPaASTM D412
    300% strain 9.65MPaASTM D412
Tensile Strength (Yield)17.2MPaASTM D412
Tensile Elongation (Break)400%ASTM D412
Compression Set 29%ASTM D395B
Bayshore Resilience 30%ASTM D2632
ThermosetNominal ValueUnit
Pot Life 7.0 - 9.0min
Demold Time (100°C)25min
Post Cure Time (100°C)4.0hr
Additional Information
Durometer Hardness, ASTM D2240, Shore A: 81 to 84Die C Tear, ASTM D1004: 215 pliAverage Split Tear, ASTM D1938: 65 pliStoichiometry Curative Level: 95%Cure Time, 150 to 160°F: OvernightMix Temperature: Andur 8200 AP: 160-212°F Curene 442: 250°F
Resin Grade Manufacturer Category Trademark
Qenos PE GM5049B Qenos Pty Ltd HDPE, HMW Qenos PE
ARC ARC66G13 ARC Resin Corporation Nylon 66 ARC
Ferro PP NPP00GW35HB Ferro Corporation PP, Unspecified Ferro PP
Kpren 135A Shandong Xuye New Materials Co., Ltd. CPE Kpren