HX-064AN is a fully-crosslinked thermoplastic elastomer(TPE) product. TPEs can be easily processed with general thermoplastic processing equipments. It has low compression set, good weatherability and excellent resistance to high temperature, chemicals, and ozone. Flexible PVC, rubbers (CR, NBR, EPDM etc.) can be replaced with TPE. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 0.970 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A) | 64 | ASTM D2240 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (100% Strain) | 2.94 | MPa | ASTM D412 |
| Tensile Strength (Break) | 6.57 | MPa | ASTM D412 |
| Tensile Elongation (Break) | 480 | % | ASTM D412 |
| Tear Strength | 24.5 | kN/m | ASTM D624 |
| Compression Set (70°C, 72 hr) | 28 | % | ASTM D395 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact (-40°C) | No Break | ASTM D256 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| MAZMID B 150 SK40 | Mazzaferro Indústria e Comércio de Polímeros e Fibras Ltda. | Nylon 6 | MAZMID B |
| RTP 3400-3 TFE 20 | RTP Company | LCP | RTP |
| Novamid® 2934A | DSM Engineering Plastics | Nylon 66/6 | Novamid® |
| Axiall PVC 1501 Clear 7002 | Axiall Corporation | PVC, Flexible | Axiall PVC |
| LUBEMID A26 GF25 NATURAL | LUBEN PLAST srl | Nylon 66 | LUBEMID |