Radiflam® S RV250FR 339 E NER

Category: Nylon 6 , Polyamide 6
Manufacturer: Radici Plastics
Trademark: Radiflam®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: RfKfPd_Radiflam-S-RV250FR-339-E-NER.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
PA6 flame retardant injection moulding grade, halogen and phosphorus free. 25% glass fiber reinforced. Deep black colour.

Suitable for parts requiring fire retardancy along with medium stiffness and good mechanical resistance. Low smoke toxicity and optical density. Applications in underground railway sector. Rated V-0 according to UL-94.

ISO 1043 : PA6 GF25 FR(61)
General Information
Filler / Reinforcement
  • Glass Fiber, 25% Filler by Weight
Additive
  • Flame Retardant
Features
  • Flame Retardant
  • Halogen Free
  • Low (to None) Phosphorus Content
  • Low Optical Density
  • Low Toxicity
RoHS Compliance
  • RoHS Compliant
UL File Number
  • E116324
Appearance
  • Black
Processing Method
  • Injection Molding
Multi-Point Data
  • Isothermal Stress vs. Strain (ISO 11403-1)
Resin ID (ISO 1043)
  • PA6 GF25 FR(61)
PhysicalDryConditionedUnitTest Method
Density 1.68--g/cm³ISO 1183
Water Absorption ISO 62
     Saturation, 23°C, 2.00 mm 2.5--%
     Equilibrium, 23°C, 2.00 mm, 50% RH 1.1--%
MechanicalDryConditionedUnitTest Method
Tensile Modulus 1450011000MPaISO 527-2/1A/1
Tensile Stress (Break)140105MPaISO 527-2/1A/5
Tensile Strain (Break)1.81.9%ISO 527-2/1A/5
Flexural Modulus 114000--MPaISO 178
Flexural Stress 2220--MPaISO 178
ImpactDryConditionedUnitTest Method
Charpy Notched Impact Strength ISO 179/1eA
     -30°C 4.0--kJ/m²
     23°C 4.56.5kJ/m²
Charpy Unnotched Impact Strength ISO 179/1eU
     -30°C 25--kJ/m²
     23°C 3540kJ/m²
ThermalDryConditionedUnitTest Method
Heat Deflection Temperature
     0.45 MPa, Unannealed 215--°CISO 75-2/Bf
     1.8 MPa, Unannealed 200--°CISO 75-2/Af
Vicat Softening Temperature 205--°CISO 306/B50
Melting Temperature 3220--°CISO 11357
ElectricalDryConditionedUnitTest Method
Surface Resistivity 1.0E+121.0E+10ohmsIEC 60093
Volume Resistivity 1.0E+151.0E+13ohms·cmIEC 60093
Comparative Tracking Index 550--VIEC 60112
FlammabilityDryConditionedUnitTest Method
Burning Rate 0.0--mm/minFMVSS 302
Flame Rating (1.60 mm)V-0--UL 94
Glow Wire Flammability Index IEC 60695-2-12
     1.00 mm 960--°C
     2.00 mm 960--°C
Glow Wire Ignition Temperature IEC 60695-2-13
     1.00 mm 725--°C
     2.00 mm 725--°C
InjectionDryUnit
Drying Temperature - Desiccant Dryer 80.0°C
Drying Time - Desiccant Dryer 2.0 to 4.0hr
Dew Point - Desiccant Dryer < -20.0°C
Suggested Max Moisture 0.10%
Processing (Melt) Temp 260 to 290°C
Mold Temperature 80.0 to 90.0°C
Injection Rate Moderate-Fast
Note Message
1 .2.0 mm/min
2 .2.0 mm/min
3 .10°C/min
Resin Grade Manufacturer Category Trademark
Regis® 6500 Noble Polymers Polyolefin, Unspecified Regis®
Tecodur® PB70 GR20 NL100 XA20 Eurotec Engineering Plastics PBT Tecodur®