apilon 52® A-6505

Category: TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester)
Manufacturer: API SpA
Trademark: apilon 52®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: RLiDGx_apilon-52-A-6505.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
apilon 52®A- 6505 is a thermoplastic polyurethane elastomer (polyester)(TPU-polyester) product,. It can be processed by extrusion or injection molding and is available in Europe. apilon 52®The application fields of A- 6505 include engineering/industrial accessories, electrical/electronic applications, electrical appliances, tools and home applications.

Features include:
  • environmental protection/green
  • Good UV resistance
  • Good flexibility
  • low temperature resistance
  • chemical resistance
General Information
Features
  • Flexibility at low temperatures
  • Good UV resistance
  • Recyclable materials
  • Good wear resistance
  • Low temperature resistance
  • Hydrolysis resistance
  • Oil resistance
Uses
  • Handle
  • Wheels
  • Conveyor belt repair
  • Electrical/Electronic Applications
  • Electrical appliances
  • Washer
  • Power/other tools
  • Pipe fittings
  • Household goods
  • Sporting goods
  • Coating application
  • Footwear
Forms
  • Particle
Processing Method
  • Extrusion
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.17g/cm³ASTM D792
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shore D, 3 sec)68ASTM D2240
MechanicalNominal ValueUnitTest Method
Tensile Strength ASTM D638
    -- 30.0MPaASTM D638
    100% strain 2.70MPaASTM D638
    300% strain 5.10MPaASTM D638
Tensile Elongation (Break)780%ASTM D638
Abrasion Resistance 50.0mm³DIN 53516
ElastomersNominal ValueUnitTest Method
Tear Strength 165.0kN/mASTM D624
InjectionNominal ValueUnit
Drying Temperature 80.0 - 110°C
Drying Time 2.0hr
Suggested Max Moisture 0.070%
Rear Temperature 180 - 190°C
Middle Temperature 185 - 200°C
Front Temperature 190 - 215°C
Nozzle Temperature 200 - 230°C
Mold Temperature 30.0 - 60.0°C
Injection Pressure 50.0 - 100MPa
Injection Rate Slow-Moderate
Injection instructions
Back Pressure: Medium to LowLocking Pressure: High
ExtrusionNominal ValueUnit
Drying Temperature 80.0 - 110°C
Drying Time 2.0hr
Suggested Max Moisture 0.070%
Cylinder Zone 1 Temp. 160 - 185°C
Cylinder Zone 2 Temp. 170 - 200°C
Cylinder Zone 3 Temp. 175 - 210°C
Cylinder Zone 4 Temp. 180 - 220°C
Die Temperature 170 - 210°C
Extrusion instructions
L/D Ratio: 20:1 to 30:1Compression Ratio: 1:2.5 to 1:3
Note Message
1 .Without Notch
Resin Grade Manufacturer Category Trademark
RTP 2740 U-70A RTP Company SBS RTP
PRIMALENE WPP551E27 Southern Polymer, Inc. EVA PRIMALENE
RTP 1007 HI UV RTP Company PBT RTP
InnoPlus LL9640A PTT Global Chemical Public Company Limited LLDPE InnoPlus
Loyblend® TK-1000 Colour Image Plastic Compound Sdn. Bhd. (CIPC) PC+PET Loyblend®