Category: | SBS , Styrene Butadiene Styrene Block Copolymer |
Manufacturer: | Franplast S.r.l. |
Trademark: | Franprene |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | RCaUwx_Franprene-TGA-2255RY.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
SBS based compound, ideal for PP over-moulding in food contact applications. It provides the item with good grip and surface soft touch. Application:
|
General Information | |
---|---|
Features |
|
Uses |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.10 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 90 | g/10 min | ASTM D1238 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Shore Hardness (Shore A) | 55 | ISO 868 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (Break) | 3.40 | MPa | ISO 527-2 |
Nominal Tensile Strain at Break | 660 | % | ISO 527-2 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tear Strength | 23 | kN/m | ISO 34-1 |
Thermal | Nominal Value | Unit | |
---|---|---|---|
Service Temperature | -30 to 70 | °C |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Time | 0.0 | hr | |
Rear Temperature | 165 to 185 | °C | |
Middle Temperature | 170 to 190 | °C | |
Front Temperature | 175 to 195 | °C | |
Nozzle Temperature | 180 to 200 | °C | |
Mold Temperature | 30.0 to 40.0 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Sylvin 8319-88FUV Orange 598 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
Bergamid™ A700 G30 H | PolyOne Corporation | Nylon 66 | Bergamid™ |
Borealis PE CG9620 | Borealis AG | HDPE | Borealis PE |
APEX® 3080 | Teknor Apex Company | PVC, Flexible | APEX® |
Sylvin 5132-86 Clear 8373 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |