| Category: | PP Copolymer , Polypropylene Copolymer |
| Manufacturer: | EMAS Plastik San.Tic.AS. |
| Trademark: | EMOPLEN® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | RATIGw_EMOPLEN-CP-MTF-30.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Polypropylene copolymer %30 talcum filled |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.10 to 1.15 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 3.0 to 20 | g/10 min | ISO 1133 |
| Molding Shrinkage | 0.85 to 1.0 | % |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Shore Hardness (Shore D) | 65 to 70 | ISO 868 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 2500 to 4000 | MPa | ISO 527-2 |
| Tensile Stress (Yield) | 30.0 to 50.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | > 10 | % | ISO 527-2 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength | > 6.0 | kJ/m² | ISO 180/1A |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 105 | °C | ISO 75-2/A |
| Vicat Softening Temperature | 100 | °C | ISO 306/B |
| Melting Temperature (DSC) | 160 | °C | ISO 3146 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| VESTODUR® GK30 | Evonik Industries AG | PBT | VESTODUR® |
| TRIREX® Compound 3025NB | Samyang Corporation | PC | TRIREX® Compound |
| Elastocon® STK40B | Elastocon TPE Technologies | TPE | Elastocon® |
| Hax™ HFX 035/3 | Fainplast Compounds S.r.l | Polyolefin, Unspecified | Hax™ |
| ESTADIENE 2020 MT | Cossa Polimeri S.r.l. | ABS | ESTADIENE |