Message |
---|
Warning: The status of this material is 'Commercial: Limited Issue' The data for this material has not been recently verified. Please contact RTP Company for current information prior to specifying this grade. |
General Information | |
---|---|
Filler / Reinforcement |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.21 | g/cm³ | ASTM D792 |
Molding Shrinkage - Flow (3.18 mm) | 0.30 | % | ASTM D955 |
Water Absorption (23°C, 24 hr) | 0.12 | % | ASTM D570 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Rockwell Hardness (R-Scale) | 118 | ASTM D785 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 5520 | MPa | ASTM D638 |
Tensile Strength | 82.7 | MPa | ASTM D638 |
Tensile Elongation (Break) | 3.5 | % | ASTM D638 |
Flexural Modulus | 4140 | MPa | ASTM D790 |
Flexural Strength | 124 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (3.18 mm) | 64 | J/m | ASTM D256 |
Unnotched Izod Impact (3.18 mm) | 640 | J/m | ASTM D4812 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Deflection Temperature Under Load | ASTM D648 | ||
0.45 MPa, not annealed | 146 | °C | ASTM D648 |
1.8 MPa, not annealed | 141 | °C | ASTM D648 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Volume Resistivity | 1.0E+10 | ohms·cm | ASTM D257 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating (1.59 mm) | V-1 | UL 94 |
Additional Information |
---|
The value listed as Flammability, UL 94, was tested in accordance with RTP test standards.Mold Shrinkage, Linear-Flow, ASTM D-955, 0.25in: 4mil/in |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 121 | °C | |
Drying Time | 4.0 | hr | |
Suggested Max Moisture | 0.020 | % | |
Suggested Max Regrind | 20 | % | |
Rear Temperature | 288 - 343 | °C | |
Middle Temperature | 288 - 343 | °C | |
Front Temperature | 288 - 343 | °C | |
Mold Temperature | 65.6 - 121 | °C | |
Injection Pressure | 68.9 - 103 | MPa |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Shandong Aobang TPU-Polyester 90-A | Shandong Aobang Chemical Technology Co.,Ltd. | TPU-Polyester | Shandong Aobang TPU-Polyester |
Unichem 7811D-02 | Colorite Polymers | PVC, Unspecified | Unichem |
Baydur® 263 IMR (600 g/m² Glass Weight) | Covestro - PUR | PUR-MDI | Baydur® |
Hylon® N2007HL | Ravago Manufacturing Americas, LLC | Nylon 6 | Hylon® |
PLEXIGLAS® Tube XT | Evonik Industries AG | Acrylic (PMMA) | PLEXIGLAS® Tube |