Category: | TP, Unspecified , Thermoplastic |
Manufacturer: | Crosspolimeri S.p.A. |
Trademark: | FRAGOM |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | Qm112T_FRAGOM-PR-04-AFKK.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
FRAGOM : is our thermoplastic compound low flame propagation in fire conditions PVC free and heavy-metal free. FRAGOM PR/04 AFKK : it is studied to extrude insulation at high speed,compound without migration risks (plasticizers-free). Meet NORMA AS.NZL 3808.2000 Insulation Type HFI-75-TP,HFI-90-TP,HFI-110-TP Sheathing Type HFS-75-TP,HFS-90-TP,HFS-110-TP Certify : CEI2011 M1,VDE0207HM4(K=0,7),BS7655 LTS 3-4 |
General Information | |
---|---|
Features |
|
Uses |
|
Agency Ratings |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.40 | g/cm³ | ASTM D792 |
Melt Mass-Flow Rate (MFR) (160°C/21.6 kg) | 8.0 | g/10 min | ASTM D1238 |
Water absorption rate- 24 hr (100°C) | 18.0 | g/m² | IEC 60811 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Hot pressing test- 6 h at 90°C-Penetration | % | IEC 60811 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Halogen Content | 0 | % | IEC 60754-1 |
Temperature Index (Combustion) 1 | > 300 | °C | NES 715 |
Corrosive gases in flue gas- pH | > 4.50 | IEC 60754-2 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Head Temperature | 185 | °C |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore D) | 55 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | > 11.0 | MPa | IEC 60811 |
Tensile Strain (Break) | > 170 | % | IEC 60811 |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Change in Tensile Strength in Air (110°C, 168 hr) | 8.0 | % | IEC 60811 |
Change in Tensile Strain at Break in Air (110°C, 168 hr) | -7.0 | % | IEC 60811 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Oxygen Index | 30 | % | ASTM D2863 |
Additional Information |
---|
No detrimental effects on properties and capability of FRAGOM in presence of convenient Masterbatch colours, black included. We suggest to dry masterbatch before using. |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 80.0 - 90.0 | °C | |
Drying Time | 3.0 - 4.0 | hr | |
Cylinder Zone 1 Temp. | 130 | °C | |
Cylinder Zone 2 Temp. | 145 | °C | |
Cylinder Zone 3 Temp. | 160 | °C | |
Cylinder Zone 4 Temp. | 180 | °C | |
Die Temperature | 190 | °C |
Note Message | |
---|---|
1 . | 21% O2 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Trithene® SX 7010 | Petroquimica Triunfo | LDPE | Trithene® |
Celanex® XFR 6842 GF30 | Celanese Corporation | PBT | Celanex® |
Chemlon® 66AT | Teknor Apex Company (Chem Polymer) | Nylon 66 | Chemlon® |
Ecomass® 1007ZC85 | Ecomass Technologies | Nylon Copolymer | Ecomass® |
POLYfill PPH T15040 | Polykemi AB | PP Homopolymer | POLYfill |