| Advanced Composites ATX904-20 is a polypropylene product, which contains 30% talc filler. It is available in North America. Typical application areas are: automotive industry. The main characteristics are: impact modification. |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Additive |
|
| Features |
|
| Uses |
|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.15 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) | 13 | g/10 min | ISO 1133 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore D) | 68 | ISO 868 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Yield) | 26.6 | MPa | ISO 527-2 |
| Flexural Modulus | 2590 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact | ISO 180 | ||
| -40°C | 2.6 | kJ/m² | ISO 180 |
| 23°C | 18 | kJ/m² | ISO 180 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature | |||
| 0.45 MPa, not annealed | 125 | °C | ISO 75-2/B |
| 1.8 MPa, not annealed | 68.4 | °C | ISO 75-2/A |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 100 | °C | |
| Drying Time | 2.0 - 4.0 | hr | |
| Rear Temperature | 193 | °C | |
| Middle Temperature | 210 - 216 | °C | |
| Front Temperature | 216 | °C | |
| Nozzle Temperature | 210 | °C | |
| Processing (Melt) Temp | 199 - 249 | °C | |
| Mold Temperature | 40.0 - 50.0 | °C | |
| Injection Rate | Slow-Moderate | ||
| Cushion | 6.35 - 12.7 | mm |
| Injection instructions |
|---|
| Injection Pressure: 50 to 60% of machine capacityScrew RPM: 1 to 2 secs before mold open |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Riblene® GP 26 | Versalis S.p.A. | LDPE | Riblene® |
| Polyopt® LM11 | Suzhou OMAY Optical Materials Co., Ltd | Film, PMMA | Polyopt® |
| GAPEX® HP RPP20EV10HB | Ferro Corporation | PP Copolymer | GAPEX® HP |
| Hiprolon® 70 NN LM | Arkema | Nylon 610 | Hiprolon® |
| Infino NH-1230U | LOTTE ADVANCED MATERIALS CO., LTD. | PC+ABS | Infino |