Category: | Epoxy , Epoxy; Epoxide |
Manufacturer: | Vyncolit N.V. |
Trademark: | Vyncolit® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | QNQ5Td_Vyncolit-E-264H.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Vyncolit E 264H is an epoxy; Epoxy resin material contains long glass fiber as filler. This product is available in North America, Africa and the Middle East, Latin America, Europe or Asia Pacific. The processing method is: resin transfer molding or compression molding. The main features of Vyncolit E 264H are:
Typical application areas include:
|
General Information | |
---|---|
Filler / Reinforcement |
|
Features |
|
Uses |
|
Agency Ratings |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.89 | g/cm³ | ASTM D792 |
Bulk Factor | 7.0 | ASTM D1895 | |
Molding Shrinkage - Flow (Transfer Molded) | 0.10 | % | ASTM D955 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Rockwell Hardness (M-Scale) | 105 | ASTM D785 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | 103 | MPa | ASTM D638 |
Flexural Modulus | 24800 | MPa | ASTM D790 |
Flexural Strength | 269 | MPa | ASTM D790 |
Compressive Strength | 186 | MPa | ASTM D695 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact | 750 | J/m | ASTM D256A |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Deflection Temperature Under Load (1.8 MPa, Unannealed) | 250 | °C | ASTM D648 |
Thermal Conductivity | 0.42 | W/m/K | ASTM C177 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Dielectric Strength | ASTM D149 | ||
-- 1 | 13 | kV/mm | ASTM D149 |
-- 2 | 12 | kV/mm | ASTM D149 |
Dielectric Constant (1 MHz) | 5.80 | ASTM D150 | |
Dissipation Factor (1 MHz) | 0.017 | ASTM D150 | |
Arc Resistance | 120 | sec | ASTM D495 |
Injection instructions |
---|
Gauge: 0.3The value listed as Thermal Conductivity, ASTM C177, was tested in accordance with ASTM F433.Water Absorption, ASTM D570, 48 hrs, 50°C: 0.15%Dielectric Strength, ASTM D149, 60 Hz, Method A, wet: 325 V/milDielectric Strength, ASTM D149, 60 Hz, Method A, dry: 375 V/milDielectric Strength, ASTM D149, 60 Hz, Method B, wet: 300 V/milDielectric Strength, ASTM D149, 60 Hz, Method B, dry: 325 V/milDielectric Constant, ASTM D150, 1000000 Hz, dry: 5.8Dissipation Factor, ASTM D150, 1000000 Hz, dry: 0.017Bulk Factor, ASTM D1895: 6 to 8Compression and Transfer Molding Conditions: Preheat Temperature: 200 to 225 °F Mold Temperature: 270 to 330 °F Compression Mold Pressure: 1000 to 8000 psi Transfer Mold Pressure: 2500 to 8000 psi Cure Time, 0.125 in: 150 to 300 sec |
Note Message | |
---|---|
1 . | Method A (short time) |
2 . | Method B (step by step) |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Nylfor® 74S5251PO 0001 | SO.F.TER. SPA | Nylon 66 | Nylfor® |
Ferro PP NPP00GT17UL WHITE | Ferro Corporation | PP, Unspecified | Ferro PP |
Polidan® T/A-LV | Solvay Specialty Polymers | XLPE | Polidan® |
POLYCOMPO PE 5305E | POLYCOMPO Co.,Ltd. | HDPE | POLYCOMPO PE |
RONFALIN® ABS 1361 | A. Schulman Europe | ABS | RONFALIN® |