| Category: | TPU, Unspecified , Thermoplastic Polyurethane Elastomer |
| Manufacturer: | Infinity LTL Engineered Compounds |
| Trademark: | INCOLOR |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | PkMqzf_INCOLOR-TPE45AOM.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| TPE 45A SHORE HARDNESS FOR CHEMICAL BOND OVERMOLD OF ABS, PC, PC/ABS, PROPIONATE, ACRYLIC AND NYLONS |
| General Information |
|---|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 0.978 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A) | 45 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength (Break) | 4.14 | MPa | ASTM D638 |
| Tensile Elongation (Yield) | 750 | % | ASTM D638 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tear Strength | 24.5 | kN/m | ASTM D624 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 68.3 - 71.1 | °C | |
| Drying Time | 4.0 | hr | |
| Rear Temperature | 185 - 191 | °C | |
| Middle Temperature | 193 - 199 | °C | |
| Front Temperature | 196 - 202 | °C | |
| Back Pressure | 0.345 - 0.689 | MPa | |
| Screw L/D Ratio | 20.0:1.0 |
| Injection instructions |
|---|
| Screw Speed: Medium to Fast |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Bormed™ HD850MO | Borealis AG | PP Homopolymer | Bormed™ |
| CERTENE™ LDF-0221J | Muehlstein | LDPE | CERTENE™ |
| Estane® 58881 TPU | Lubrizol Advanced Materials, Inc. | TPU-Polyether | Estane® |
| LEXAN™ 940 resin | SABIC Innovative Plastics | PC | LEXAN™ |
| LEXAN™ EXL9112 resin | SABIC Innovative Plastics | PC | LEXAN™ |