RTP 507

Category: SAN , Styrene Acrylonitrile
Manufacturer: RTP Company
Trademark: RTP
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: PMFclU_RTP-507.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Glass Fiber
General Information
Filler / Reinforcement
  • Glass fiber reinforced material, 40% filler by weight
RoHS Compliance
  • Contact manufacturer
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.40g/cm³ASTM D792
Molding Shrinkage - Flow (3.20 mm)0.050 - 0.15%ASTM D955
MechanicalNominal ValueUnitTest Method
Tensile Modulus 13100MPaASTM D638
Tensile Strength 124MPaASTM D638
Tensile Elongation (Yield)1.0 - 2.0%ASTM D638
Flexural Modulus 12400MPaASTM D790
Flexural Strength 172MPaASTM D790
ImpactNominal ValueUnitTest Method
Notched Izod Impact (3.20 mm)48J/mASTM D256
Unnotched Izod Impact (3.20 mm)210J/mASTM D4812
FlammabilityNominal ValueTest Method
Flame Rating (1.50 mm, ** Values per RTP Company testing.)HBUL 94
Additional InformationNominal ValueUnit
Primary Additive 40%
InjectionNominal ValueUnit
Drying Temperature 82.2°C
Drying Time 2.0hr
Processing (Melt) Temp 238 - 279°C
Mold Temperature 51.7 - 82.2°C
Injection Pressure 68.9 - 103MPa
Injection instructions
Desiccant Type Dryer Required.
Resin Grade Manufacturer Category Trademark
RTP 2101 HF RTP Company PEI RTP
Shandong PA1212 GYBHVN Shandong Guangyin New Materials Co., Ltd. Nylon 1212 Shandong PA1212