| Category: | EVA , Ethylene Vinyl Acetate Copolymer Resin |
| Manufacturer: | ExxonMobil Chemical |
| Trademark: | Escorene™ Ultra |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | PFwCmP_Escorene-Ultra-UL-00014.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| UL 00014 is a copolymer of ethylene and vinyl acetate. |
| General Information | |
|---|---|
| Additive |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 0.25 | g/10 min | ASTM D1238 |
| Vinyl Acetate Content | 14.0 | wt% | ExxonMobil Method |
| Films | Nominal Value | Unit | Test Method |
|---|---|---|---|
| secant modulus | ASTM D882 | ||
| 1% secant, MD | 65.0 | MPa | ASTM D882 |
| 1% secant, TD | 68.0 | MPa | ASTM D882 |
| Tensile Strength | ASTM D882 | ||
| MD : Fracture | 33.0 | MPa | ASTM D882 |
| TD : Fracture | 35.0 | MPa | ASTM D882 |
| Tensile Elongation | ASTM D882 | ||
| MD : Fracture | 610 | % | ASTM D882 |
| TD : Fracture | 670 | % | ASTM D882 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Vicat Softening Temperature | 76.0 | °C | ASTM D1525 |
| Legal statement |
|---|
| 有关潜在食品接触应用合规信息(例如:FDA、EU、HPFB),请与埃克森美孚化工客户服务代表联系。本产品不宜在医疗应用中使用,亦不应在任何此类应用中使用 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| PrimoPrene 60A-1000 | KMI Group Inc. | TPV | PrimoPrene |
| Elastron® D D100.A50.B | Elastron USA, Inc. | SBS | Elastron® D |
| Epolene® N-14 | Westlake Chemical Corporation | LDPE | Epolene® |
| ISOTHANE® 3060A | Great Eastern Resins Industrial Co Ltd (GRECO) | TPU-Polyether | ISOTHANE® |
| PPR POM17 | Premier Plastic Resins, Inc. | Acetal (POM) Homopolymer | PPR |