Category: | Nylon 6 , Polyamide 6 |
Manufacturer: | Grupo Repol |
Trademark: | DINALON® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | P7ptyt_DINALON-B1S35-V2-7035.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
DINALON® B1S35 V2-7035 is a Polyamide 6 (Nylon 6) product. It is available in Europe. Characteristics include:
|
General Information | |
---|---|
Features |
|
Appearance |
|
Forms |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.16 | g/cm³ | ISO 1183/A |
Humidity 1 | < 0.25 | % | ISO 15512/B |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 3200 | MPa | ISO 527-2 |
Tensile Stress (Break) | 80.0 | MPa | ISO 527-2 |
Tensile Strain (Break) | 25 | % | ISO 527-2 |
Flexural Modulus | 2500 | MPa | ISO 178 |
Flexural Stress | 100 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength (23°C) | 3.0 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength (23°C) | No Break | ISO 179/1eU |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 50.0 | °C | ISO 75-2/A |
Vicat Softening Temperature | > 200 | °C | ISO 306/B |
Flammability | Nominal Value | Test Method | |
---|---|---|---|
Flame Rating (1.60 mm) | V-2 | UL 94 |
Note Message | |
---|---|
1 . | Karl-Fischer |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
TITANLENE® LDF 204GH | Lotte Chemical Titan (M) Sdn. Bhd. | LDPE | TITANLENE® |
Electrafil® POM CF15 | Techmer Engineered Solutions | Acetal (POM) Copolymer | Electrafil® |
Lupoy® 1080-70 | LG Chem Ltd. | PC | Lupoy® |
WELLAMID Nylon 6600/42 GS 30 HWCP | CP-Polymer-Technik GmbH & Co. KG | Nylon 66 | WELLAMID Nylon |
Sylvin 9077-75C NATURAL | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |