Category: | Nylon 66/6 , Polyamide 66/6 Copolymer |
Manufacturer: | Solvay Engineering Plastics |
Trademark: | TECHNYL® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | P1nB2x_TECHNYLB218V20BLACK21N.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
TECHNYL® B 218 V20 Black 21N is a polyamide 66/6, reinforced with 20% of glass fibre, heat stabilized, for injection moulding. This grade offers an excellent combination between impact resistance, rigidity, thermal resistance and surface appearance. |
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Uses |
|
Agency Ratings |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Resin ID (ISO 1043) |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.28 | -- | g/cm³ | ISO 1183/A |
Water Absorption | ISO 62 | |||
23°C, 24 hr | 1.2 | -- | % | ISO 62 |
Equilibrium, 23°C, 50% RH | 2.7 | -- | % | ISO 62 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus (23°C) | 7500 | 5000 | MPa | ISO 527-2/1A |
Tensile Stress (Break, 23°C) | 140 | 85.0 | MPa | ISO 527-2/1A |
Tensile Strain (Break, 23°C) | 3.0 | 9.0 | % | ISO 527-2 |
Flexural Modulus (23°C) | 6000 | 3500 | MPa | ISO 178 |
Flexural Stress (23°C) | 230 | -- | MPa | ISO 178 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength (23°C) | 7.0 | 9.0 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength (23°C) | 45 | 83 | kJ/m² | ISO 179/1eU |
Notched Izod Impact (23°C) | 8.0 | 13 | kJ/m² | ISO 180 |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 230 | -- | °C | ISO 75-2/Af |
Melting Temperature | 242 | -- | °C | ISO 11357-3 |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Surface Resistivity | 6.0E+15 | 1.0E+14 | ohms | IEC 60093 |
Volume Resistivity | 1.0E+15 | 1.0E+14 | ohms·cm | IEC 60093 |
Dielectric Strength (2.00 mm) | 32 | 28 | kV/mm | IEC 60243-1 |
Dissipation Factor | 0.010 | 0.11 | IEC 60250 | |
Comparative Tracking Index (Solution A) | 450 | 350 | V | IEC 60112 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Oxygen Index | 23 | -- | % | ISO 4589-2 |
Injection | Dry | Unit | |
---|---|---|---|
Drying Temperature | 80 | °C | |
Suggested Max Moisture | 0.20 | % | |
Rear Temperature | 255 - 265 | °C | |
Middle Temperature | 260 - 270 | °C | |
Front Temperature | 270 - 280 | °C | |
Mold Temperature | 70 - 100 | °C |
Injection instructions |
---|
The material is supplied in airtight bags, ready for use. In case that the virgin material has absorbed moisture, it must be dried with a dehumidified air drying equipment, dew point mini -20°C. Recommended time 2-4hInjection Advice: For reinforced polyamide, Solvay recommends the use of steel with a high content of Carbon and purified for polishing to avoid or limit the abrasion. For example: X38CrMoV5-1 (EN Norm) - 1.2367 /1.2343 (DIN Norm) or X160CrMoV12 (EN Norm) - 1.2601 /1.2379 (DIN Norm). For Mould Temperature, in the case of parts where the surface roughness is required we can recommend a temperature of 90°C to 120°C with an optimum at 105°C. The processing parameters like processing temperatures are a recommendation and can be adjusted in function of injection machine size, part geometry / design |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 282 TFE 10 | RTP Company | Nylon 66 | RTP |
MTEGRITY™ LLDPE LL108AA | M. Holland Company | LLDPE | MTEGRITY™ LLDPE |
Amilan® CM1061 | Toray Resin Company | Nylon 6 | Amilan® |
KYOCERA TCG1180K2 | KYOCERA Chemical Corporation | TS, Unspecified | KYOCERA |
Plaslube® PEEK CF10 GL10 TL10 A HF | Techmer Engineered Solutions | PEEK | Plaslube® |